Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 991 - 3050 microns | 39.0 - 120 mil | Range of Thicknesses Available |
Rogers Corporation Poron® 4790-92-15 Supported Urethane Foam, Extra Soft, Slow Rebound, PET Reinforced Extra soft, slow rebound with a very low closure force.Features and Benefits of PORON Products: Excellent compression set resistance which enables durable, long-term performance for gasketing, seali.. |
|||
Thickness | 127 - 3050 microns | 5.00 - 120 mil | Range of Standard Thicknesses |
Rogers Corporation RT/duroid® 6002 High Frequency Laminate Features:Low loss for excellent high frequency performanceTight dielectric constant and thickness controlExcellent electrical and mechanical propertiesExtremely low thermal coefficient of dielectric.. |