Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2030325D14 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Möller Medical NanoSkin 78 NanoCoating Transparent, scratch-resistant coating also for plastics with good resistance against dissolvents.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Möller Medical PolySkin 81 NanoCoating Flexible, non-abrasive, decorative coating; easy-to-clean effect can be addedInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | |
Möller Medical TafSkin 103 NanoCoating Highly flexible, non-abrasive, chemical-resistant PTFE coating with very good easy-to-clean properties, biocompatible.Information provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2050425D1 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | Using a 230 stainless steel mesh screen |
Gwent Electronic Materials C2110817D5 Conductive Silver Polymer Paste This product is a thermoplastic screen printing ink, developed for use in membrane touch switch applications as well as counter electrode in electro-chemical sensors and conductive tracks. It may b.. |
|||
Thickness | 10.0 - 30.0 microns | 0.394 - 1.18 mil | cured |
Gwent Electronic Materials C2121119D9 Nanocopper based Paste This product is a nanocopper based paste that is designed for flat bed screens. The product is compatible with printing on PET substrates such as the DuPont Melinex ST-505. Produced using nano-par.. |
|||
Thickness | 15.0 - 30.0 microns | 0.591 - 1.18 mil | |
Dow CYCLOTENE™ XU35075 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35075 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2040226D2 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |
|||
Thickness | 20.0 - 30.0 microns | 0.787 - 1.18 mil | |
Gwent Electronic Materials C2040226D4 Curable Carbon Ink This product is based on a unique curing process that results in the low temperature formation of a thermosetting conductive coating that combines good adhesion with excellent chemical, solvent and .. |