Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 15.2 - 203 microns | 0.600 - 8.00 mil | Average value: 57.4 microns Grade Count:12 |
Overview of materials for Polychlorotrifluoroethylene; Molded This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu.. |
|||
Thickness | 152 - 203 microns | 6.00 - 8.00 mil | |
3M Scotchkote™ XF 895 Fast Curing Floor Coating Scotchkote Fast Curing Floor Coating XF 895 has been specifically developed as a high build floor protection system for application to concrete surfaces, to provide rapid return to serviceProduct Fe.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-10 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-14 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-64 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-71 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-72 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-75 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-76 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-77 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-81 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-82 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-85 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ IJ680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ RG680-10 Reflective Graphic Film 6-mil flexible, enclosed lens, retroreflective films; Available in white only; Similar daytime and nighttime appearance that retains most of its reflectivity when wet; Excellent angularity; Pressure.. |
|||
Thickness | 127 - 203 microns | 5.00 - 8.00 mil | Side 1 |
Arlon 44250R011 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wri.. |
|||
Thickness | 152 - 203 microns | 6.00 - 8.00 mil | Side 1 |
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 165 - 203 microns | 6.50 - 8.00 mil | Overall |
Arlon 45561R007 0.007"(0.178 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured RubberAppearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The data should not .. |