Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 25.4 - 102 microns | 1.00 - 4.00 mil | Range of Standard Thicknesses |
Rogers Corporation Ultralam® 3850 Liquid Crystalline Polymer Circuit Material ULTRALAM® 3850 laminate circuit materials utilize highly temperature resistant liquid crystalline polymer (LCP) as the dielectric film.Features & Benefits:Excellent high frequency propertiesStable .. |
|||
Thickness | 25.4 - 102 microns | 1.00 - 4.00 mil | |
Alcoa KAMA 2100 Prime Clear OPS, Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Thickness | 25.4 - 102 microns | 1.00 - 4.00 mil | |
Alcoa KAMA 2500 Prime Clear OPS, Shrink Film
(discontinued **) CapabilitiesGauge: .001” to .004” (28 to 101µm)Width: .2” to 80” (50.8 to 2032mm)Core size: 3” and 6” standard cores, 8” availableRoll O.D.: various confiations availableCustom colors and ti.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ 180Cv2-10 Graphic Film with Comply™ Adhesive 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Conforms to flat surfaces, with and without ri.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-77 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-015 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-156 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-246 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-25 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-33 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3650-10 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-14 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-23 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000LF-10 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000LF-13 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ RG3650-114 Graphic Film 2-mil, opaque white and transparent film; Pressure-sensitive adhesive; Permanent filmInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ RG180-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ RG180C-10 Graphic Film 2-mil white, vinyl film with a luster finish; Excellent hiding power; Pressure-activated adhesive for easy sliding, tacking, snap up and repositioning; Flexible; conforms to compound cures, corrugat.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-11 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-14 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-157 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-49 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3650-12 Graphic Film 2-mil opaque film; Available in white, black and transparent; Pressure-sensitive adhesive; Resists gasoline vapors and occasional petroleum spills; Permanent filmInformation provided by 3M |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 8000-37 Graphic Film This 2-mil, screen printable film with a pressure sensitive adhesive that can be used on flat and simple curved surfaces. This film withstands severe weather dn handling conditions encountered by co.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Controltac™ 8620C ES Changeable Graphic Film with Comply™ Adhesive These 2 mil films offer versatility along with sideable, repositionable, pressure activated adhesive. These long term durable and removable films have excellent hiding power and stability, making th.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000-63 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 1000LF-120 Graphic Film 2-mil vinyl film; Wide color selection; Includes three colors with both a layflat liner and gray adhesive for excellent hiding power and a transparent film with a layflat liner; Pressure-sensitive a.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3232-44 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | with adhesive |
3M Scotchcal™ 3632-20 Translucent Film 2-mil translucent cast vinyl film; Matte surface finish that eliminates glare and provides uniform color in reflective light; Built in Graphic Protection System (GPS), which is a top coat that incre.. |
|||
Thickness | 76.2 - 102 microns | 3.00 - 4.00 mil | Side 2 |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |