Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thickness = 91.4 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 91.4 - 102 microns
3.60 - 4.00 mil
Range of Thicknesses available
Rogers Corporation RO4450B Prepreg
Prepreg is commonly used to inexpensively form less critical signal layers in antenna designs. A high post-cure Tg makes RO4400 series prepreg an excellent choice for multi-layers requiring sequent..
Thickness 91.4 microns
3.60 mil
Hexcel® HexForce™ 1125 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 91.4 microns
3.60 mil
ExxonMobil Label-Lyte® 90 LP Coated, High Sheen, Metallized, White Opaque OPP for Water-based Patch Label Applications
Coated, white, metallized polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement. This film is compatible with offset litho and UV-cured in..
Thickness 91.4 microns
3.60 mil
ExxonMobil Label-Lyte® 95 LP Coated, White Opaque OPP for Water-based Patch Label Applications
White, polypropylene film designed for use in water-based, wet glue, cut-and-stack, patch labeling for paper replacement on glass, metal, HDPE, and PET containers. It is designed to be used as a mon..
Thickness 91.4 microns
3.60 mil
Total; ASTM D3652
3M 33803 General Purpose Aluminum Foil Tape
High tack rubber adhesive. 40 lb liner. UL 723 ClassifiedInformation provided by 3M
Thickness 91.4 microns
3.60 mil
Total; ASTM D3652
3M 433 Premium Performance Aluminum Foil Tape
Silicone adhesive for high temperature resistance; MIL-T-47014, FAR 25.853, UL 746C Recognized; smooth easy unwind; clean, straight edges with minimal wrinkling.Information provided by 3M
Thickness 91.4 microns
3.60 mil
Liner
3M FA03J Matte Clear Acetate Label Products
3M™ Matte Clear Acetate Label Products offer consistent, high quality film appearance. This film die-cuts easily which helps extend die life in comparison with polyester label stocks. These acetate..
Thickness 91.4 microns
3.60 mil
Liner
3M FM0196J MC Polyester Label Products
3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz..
Thickness 91.4 microns
3.60 mil
Liner
3M FM118J Indoor UL Recognized MC Polyester Label Products
3M™ Indoor UL Recognized MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These po..
Thickness 91.4 microns
3.60 mil
Liner
3M FM16J Indoor UL Recognized Computer Imprintable White Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable White Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Thickness 91.4 microns
3.60 mil
Liner
3M FM28J Indoor UL Recognized White Polyester Label Products
3M™ Indoor UL Recognized White Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize 3M™ A..
Thickness 91.4 microns
3.60 mil
Total; ASTM D3652
3M 3302 Specialty Foil Tape
Aluminum foil tape. EMI/RFI shielding. Ul 510 Recognized.Information provided by 3M
Thickness 91.4 microns
3.60 mil
Total; ASTM D3652
3M 3311 General Purpose Aluminum Foil Tape
Ul 723 listedInformation provided by 3M
Thickness 91.4 microns
3.60 mil
Adhesive
3M 9453LE Adhesive Transfer Tapes with Adhesive 300LSE
3M™ Adhesive Transfer Tapes with 3M™ Low Surface Energy Acrylic Adhesive 300LSE provides high bond strength to most surfaces, including many low surface energy plastics such as polypropylene and p..
Thickness 91.4 microns
3.60 mil
Liner
3M FM0196J MC Polyester Label Product
3M™ MC Polyester Label Products are white durable, high performance micro-cavitated polyester materials that offer excellent thermal stability and moisture resistance. These polyester labels utiliz..
Thickness 91.4 microns
3.60 mil
Liner
3M FM14J Indoor UL Recognized Computer Imprintable Clear Polyester Label Product
3M™ Indoor UL Recognized Computer Imprintable Clear Polyester Label Products are durable high performance materials that offer excellent thermal stability and moisture resistance. These products ar..
Thickness 91.4 microns
3.60 mil
ASTM D3652
3M Scotch® 3311 Foil Tape
Scotch® Foil Tape 3311 is an aluminum alloy foil with a pressure-sensitive adhesive and paper liner. The aggressive rubber adhesive sticks well to most surfaces and the paper liner makes for conven..