Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 63.5 microns | 2.50 mil | Polyethylene, Interleave |
Arlon 920-410C##FR-P1 0.020" (0.508 mm) Cured Self-fusing Silicone Tape
(discontinued **) Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1” Wide Rectangular 1 inch wide, 20 mil thick, Brown, Rectangular cross-section, Self-fu.. |
|||
Thickness | 63.5 - 140 microns | 2.50 - 5.50 mil | Side 1 |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 63.5 microns | 2.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 48101R008 0.008" (0.203 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cured Silicone RubberInterleave 2: Polyethylene Product Use: Flexible heater insul.. |
|||
Thickness | 63.5 microns | 2.50 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 48106R008 0.008" (0.203 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Thickness | 63.5 microns | 2.50 mil | Side 2 |
Arlon 49581R010 0.0105" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1681 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the .. |
|||
Thickness | >= 63.5 microns | >= 2.50 mil | Side 2 |
Arlon 51591R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass with polymer release linersThis data .. |
|||
Thickness | 63.5 microns | 2.50 mil | Interleave |
Arlon 61089R040 0.040" (1.02 mm) Uncured/Cured Silicone Rubber with Denier Vectran HS Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 1000 Denier HS Appearance: Red silicone gum on fabricThis data represents t.. |
|||
Thickness | 63.5 - 140 microns | 2.50 - 5.50 mil | Side 1 |
Arlon R34896R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 63.5 microns | 2.50 mil | Total; ASTM D3652 |
3M Scotch® 824 Pouch Tape Scotch® Pouch Tape 824 is a pressure-sensitive tape with a bright, orange boarder on all four edges, and a non-tack “see-through” central rectangle, which provides a quick, simple, highly visible.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-103 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-177 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-186 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-24 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-47 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-56 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-77 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-114 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 microns | 2.50 mil | ASTM D3652 |
3M ScotchPad™ 830 Pouch Tape Pads 3M™ ScotchPad™ Pouch Tape Pads are pre-cut pressure-sensitive tapes with a sticky boarder and a printed, non-tack center section that comes either as a standard or custom printed pouch which is cl.. |
|||
Thickness | 63.5 microns | 2.50 mil | Interleave |
Arlon 48B12R005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassThis data represents typical values for the production material. The data should not be used.. |
|||
Thickness | 63.5 microns | 2.50 mil | Liner |
3M 7110 Performance Paper Label Material 3M™ Performance Paper Label Material 7110 adheres well to a variety of surfaces including high (HSE) and low surface energy (LSE) plastics and provides excellent resistance to flagging on small dia.. |
|||
Thickness | 63.5 - 114 microns | 2.50 - 4.50 mil | Side 2 |
Arlon 51971R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 63.5 microns | 2.50 mil | Interleave |
Arlon 55103R030 0.030" (0.762 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materia.. |
|||
Thickness | 63.5 microns | 2.50 mil | Interleave |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 63.5 microns | 2.50 mil | Interleave 2 |
Arlon R38041X012 0.012" (0.305 mm) Uncured Fluorosilicone with Fiberglass Substrate Design/Construction: Interleave 1: PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Style 2116 FiberglassSide 2: Uncured Silicone Rubber Interleave 2: Polyethylene Appearance: Gray silicone gum.. |
|||
Thickness | 63.5 microns | 2.50 mil | ASTM D3652 |
3M Scotch® 3734 Printed Message Box Sealing Tape Scotch® Box Sealing Tape 3734 is a polypropylene carton sealing tapes. A high performance box sealing tape with a strong backing and an aggressive adhesive that provides a secure and durable closur.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-307 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-53 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-357 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7725-49 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; Transparent synthetic liner resists moisture absorption and static build up; Lays flat for easier ass.. |
|||
Thickness | 63.5 - 88.9 microns | 2.50 - 3.50 mil | with adhesive |
3M Scotchcal™ ElectroCut™ 7125-88 Graphic Film 2-mil cast vinyl in 61 colors; Pressure-sensitive, permanent adhesive; Same color on both sides; The blue paper liner on 7125-10 and 7125-20 provides easier visibility when weeding, other film color.. |