Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 50800 microns | 2000 mil | |
Unifrax FyreWrap® Cable Insulation Unifrax's FyreWrap® Cable Insulation is a thin, flexible, insulation wrap designed to provide a fire-protective enclosure around cable trays and conduit. The FyreWrap system ensures electrical cir.. |
|||
Thickness | 50800 microns | 2000 mil | |
Unifrax FyreWrap® MAX 2.0 Duct Insulation Two-Layer ASTM E-2336 System Unifrax's FyreWrap® MAX 2.0 Duct Insulation is a high-temperature insulation blanket specifically designed to provide a flexible enclosure for one- and two-hour rated commercial kitchen grease duct.. |