Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 48.3 microns | 1.90 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired.Availability: Africa & M.. |
|||
Thickness | 48.3 microns | 1.90 mil | ExxonMobil Method |
ExxonMobil Label-Lyte™ 47LTL247 OPP Film Product Description: A super white opaque, high gloss, cavitated BOPP film designed for use in reel-fed wrap-around labeling applications where superior graphics are desired. 47LTL247 with supplied .. |
|||
Thickness | 48.3 microns | 1.90 mil | ExxonMobil Method |
ExxonMobil Oppalyte™ 47MW247 OPP Film Product Description: A super white opaque biaxially oriented polypropylene film. It is designed for use in cold seal applications where superior optics and graphics are desired.Availability: Africa .. |
|||
Thickness | 48.3 microns | 1.90 mil | Backing; ASTM D3652 |
3M 1450 Aluminum Foil Tape 3M™ Aluminum Foil Tape 1450 is an aluminum foil with transparent, high-tack, rubber adhesive.Information provided by 3M |
|||
Thickness | 48.3 microns | 1.90 mil | Backing; ASTM D3652 |
3M 1450 General Purpose Aluminum Foil Tape High tack adhesive for good, instant adhesion to many surfaces.Information provided by 3M |
|||
Thickness | 48.3 microns | 1.90 mil | Backing; ASTM D3652 |
3M 431 Premium Performance Aluminum Foil Tape Conformable aluminum tape. UL 723 ClassifiedInformation provided by 3M |
|||
Thickness | 48.3 microns | 1.90 mil | Backing; ASTM D3652 |
3M 439 Premium Performance Aluminum Foil Tape Linered version of 431Information provided by 3M |
|||
Thickness | 48.3 microns | 1.90 mil | Facestock |
3M 7014 Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Thickness | 48.3 microns | 1.90 mil | Facestock |
3M 7014FP Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Thickness | 48.3 microns | 1.90 mil | ASTM D3652 |
3M Highland™ 3565 Label Protection Tape 3M™ Highland™ Label Protection Tape 3565 has a clear, strong, moisture-resistant film backing and a strong adhesive that holds well to many treated and finished surfaces. It is used for the attach.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 3771 Standard Message Box Sealing Tape Scotch® Box Sealing Tape 3771 is a standard message packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consist.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 3779 Security Message Box Sealing Tape Scotch® Security Message Box Sealing Tape 3779 is an industrial packaging tape used for box sealing specifically where security of the carton contents is a concern. The printed design along with th.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 640 Transparent Film Tape Scotch® 640 is a transparent film tape used for sealing, tabbing, splicing, various inner-pack applications and garment applications. This product has a conformable backing and a consistent pressur.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 829 Packing List Pouch Tape Scotch® Packaging List Pouch Tape 829 is a pressure-sensitive tape with a red boarder framing a non-sticky, clear, rectangular center window, which allow attaching and protection of packing lists a.. |
|||
Thickness | 48.3 microns | 1.90 mil | Facestock |
3M 7014FL Performance Paper Label Material 3M™ Performance Paper Label Material provides excellent resistance to flagging on small diameter vials. These label materials utilize 3M™ High Precision Acrylic Adhesive 320, which provides firmne.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3752 |
3M 8401 Polyester Tape 3M™ Polyester Tape 8401 is designed for splicing many release coated papers.Information provided by 3M |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3752 |
3M 850 Polyester Film Tape 3M™ Polyester Film Tape 850 can generally be used for splicing and applications where chemical resistance and/or clean removal is necessary. The silver backing is a transparent polyester with a thi.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 353 High Performance Box Sealing Tape Scotch® Box Sealing Tape 351 is a high performance packaging tape used for box sealing, splicing, recouperage and other demanding packaging applications. This product has a strong abrasion resistan.. |
|||
Thickness | 48.3 microns | 1.90 mil | ASTM D3652 |
3M Scotch® 371 Industrial Box Sealing Tape Scotch® Box Sealing Tape 371 is an industrial packaging tape used for box sealing, splicing, recouperage and other packaging applications. This product has a conformable backing and a consistent pr.. |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3652 |
3M Scotch® 3781 Industrial Continuous Taping System Tape Scotch® Taping System Tape 3781 is an industrial continuous packaging tape used for box sealing and specially designed for use with the 3M-Matic™ Continuous Taping System (CTS) stand. The Product .. |
|||
Thickness | 48.3 microns | 1.90 mil | estimated wet film thickness |
Aremco Lamp-Coat™ LC4040-SG High Temperature Coating, Silicone White reflective coating for use on mercury vapor lamps and other high temperature glass and quartz components to 1200 ºF (649 ºC). |
|||
Thickness | 48.3 microns | 1.90 mil | Total; ASTM D3752 |
3M 8402 Polyester Tape 3M™ Polyester Tape 8402 is a film tape with a silicone adhesive for composite bonding and splicing of many silicone coated papers and films.Information provided by 3M |