Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 28.0 microns | 1.10 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT11 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT11 is a general, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion, good dimensional stability, and high tensile strength. One side has c.. |
|||
Thickness | 28.0 microns | 1.10 mil | ± 2.5%; ASTM-252-78 |
Kinlead PT12 Adhesive Tape Grade BOPP Plain Film (thickness: 28 µm) PT12 is a super clear, adhesive tape grade BOPP plain film. It is transparent and non heat sealable. It has excellent glue adhesion and high clarity. One side has corona treatment. It is widely used.. |
|||
Thickness | 28.0 microns | 1.10 mil | Using a 230 mesh stainless steel screen, 13 micron emulsion |
Gwent Electronic Materials C2040308D2 Silver/Silver Chloride Paste Silver/Silver Chloride Paste has a ratio of Silver to Silver Chloride of 40/60. The paste is in a ready to use form at a viscosity suitable for automatic or semi-automatic screen printing. The paste.. |