Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 270 - 750 microns | 10.6 - 29.5 mil | includes both PET and PE layers |
OCTAL DPET™/PE Laminate Sheet with Improved Barrier Properties Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Thickness | 270 - 750 microns | 10.6 - 29.5 mil | includes both PET and PE layers |
OCTAL DPET™/PE Lock-Up Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Thickness | 270 - 750 microns | 10.6 - 29.5 mil | includes both PET and PE layers |
OCTAL DPET™/PE Peelable Laminate Sheet Clear direct-to-sheet amorphous PET sheet with a polyethylene laminate film. Approved for food contact packaging. Information provided by OCTAL Petrochemicals. |
|||
Thickness | 270 microns | 10.6 mil | Nominal |
AK Steel TRAN-COR® H-1 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 270 microns | 10.6 mil | Nominal |
AK Steel TRAN-COR® H-1 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 270 - 310 microns | 10.6 - 12.2 mil | |
AK Steel TRAN-COR® H-2 CARLITE® DR® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |
|||
Thickness | 270 - 310 microns | 10.6 - 12.2 mil | |
AK Steel TRAN-COR® H-2 CARLITE® Grain Oriented Electrical Steel TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l.. |