Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 254 - 1520 microns | 10.0 - 60.0 mil | Range of Standard Thicknesses |
Rogers Corporation RT/duroid® 6035HTC Ceramic Filled PTFE Composite, High Power RF and Microwave Features & Benefits:High thermal conductivity - Improved dielectric heat dissipation, enabling lower operating temperatures for high power applicationsLow loss tangent - Excellent high frequency per.. |
|||
Thickness | 254 microns | 10.0 mil | Per Ply |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, 4581 Quartz Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Thickness | 254 microns | 10.0 mil | Per Ply |
Park Electrochemical Nelcote® E-761 Epoxy Prepreg, Spectra® 951 - PT Reinforced Nelcote® E-761 is a versatile self-adhesive epoxy matrix for use in aerospace and commercial application where ease of processing and cost are key considerations.Key Features and Benefits:Controlle.. |
|||
Thickness | 254 microns | 10.0 mil | cured laminate, per ply |
Park Electrochemical Nelcote® P-650R Polyester Prepreg, 7781 E-Glass Reinforced Nelcote® P-650R is a non-styrenated/low VOC polyester resin system that has been designed for optical clarity. P-650 exhibits good mechanical properties up to 250°F.Key Features and Benefits:Non-s.. |
|||
Thickness | >= 254 microns | >= 10.0 mil | |
Parker Chomerics CHO-BOND 360-208 Conductive Epoxy Low cost, electrically conductive epoxy adhesive that combines the good adhesive characteristics as epoxy, and the superior electrical conductivity of silver. It is recommended as a thermo-setting E.. |
|||
Thickness | 254 microns | 10.0 mil | Recommended |
Parker Chomerics CHO-BOND 589-29 Conductive Epoxy Low cost, highly conductive adhesive system which combines the strong adhesion characteristics of an epoxy with the superior conductivity of silver. CHO-BOND 589-29 adhesive meets the most exacting .. |
|||
Thickness | 254 microns | 10.0 mil | |
GrafTech eGRAF® HITHERM™ HT-710 Graphite Made from natural graphite, eGRAF® HITHERM™ thermal interface materials are designed for use in applications requiring low contact resistance and high thermal conductivity. HITHERM™ mat.. |
|||
Thickness | 254 microns | 10.0 mil | Gauge, nominal |
Mid-Mountain Materials ARMATEX® SF10 Silicone Rubber Coated Glass Fabric Description: Armatex Coatings are applied to base textiles that range in chemical composition, confiation and weight. Mid-Mountain specializes in engineered coatings, both polymer and mineral based... |
|||
Thickness | 254 microns | 10.0 mil | |
Hexcel® HexForce™ 354 Aramid Fabric Hexcel manufactures aramid fabrics for use in aerospace applications as well as marine, tooling and recreational products where high strength, low weight, and impact resistance are essential. Aramid.. |
|||
Thickness | 254 microns | 10.0 mil | Nominal |
DuPont™ Nomex® 411 Paper, 10 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Thickness | 254 microns | 10.0 mil | |
Daikin NEOFLON NF-0250 FEP Film NEOFLON FEP films are a high performance film made from NEOFLON FEP resin and have superior reliability and retention of their properties. NEOFLON FEP is applicable in such diversified fields as el.. |
|||
Thickness | 254 microns | 10.0 mil | Backing; ASTM D3652 |
3M 2552/Silver Damping Foils General purpose vibration dampingInformation provided by 3M |
|||
Thickness | 254 microns | 10.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Thickness | 254 microns | 10.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 55572XA028 0.028" (0.711 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 Fiberglass This data Represents typical values for the production material. The data should not be used to write, or in place of.. |
|||
Thickness | 254 microns | 10.0 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia.. |
|||
Thickness | 254 microns | 10.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 910-10BXX-P0 0.010" (0.254 mm) Cured Self-fusing Silicone Tape Design/Construction: Interleave: Polyethylene Rubber: Cured Self-fusing Silicone Rubber Cross Section Type: 1" Wide Rectangular 1 inch wide, 10 mil thick, Black, Rectangular cross-section, Self-fus.. |
|||
Thickness | 254 microns | 10.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 99570R010 0.010" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Liner: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and should not be us.. |
|||
Thickness | 254 microns | 10.0 mil | Side 1; Arlon SQA-TMS-003 |
Arlon 99580R010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassFlexible heater substrateAppearance: Red, High viscosity gum on release linersThis data repres.. |
|||
Thickness | 254 microns | 10.0 mil | Side 1 |
Arlon 99790N010 0.010" (0.254 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Liner: FEP Side 1: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used to write,.. |
|||
Thickness | 254 microns | 10.0 mil | Side 2; Arlon SQA-TMS-003 |
Arlon R30711R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1165 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: PolyethyleneAppearance: Red silicone gum .. |
|||
Thickness | 254 microns | 10.0 mil | |
3M Scotchkote™ 175SR Epoxy Coating Scotchkote Epoxy Coating 175SR has been specifically developed as at 100% solids lining for the internals of tanks, vessels and other equipment in contact with aromatic hydrocarbon solvents, ethanol.. |
|||
Thickness | 254 microns | 10.0 mil | |
3M Scotchkote™ 175UC Epoxy Coating Scotchkote Epoxy Coating 175UC has been specifically developed as a 100% solidsProduct Features:Combines good application characteristics with excellent corrosion protection and ultimate chemical re.. |
|||
Thickness | 254 - 305 microns | 10.0 - 12.0 mil | Overall |
Arlon 44571R010 0.011" (0.279 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |
|||
Thickness | 254 microns | 10.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricTh.. |
|||
Thickness | 254 microns | 10.0 mil | Side 2 |
Arlon 51426R020 0.020" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr.. |
|||
Thickness | 254 microns | 10.0 mil | |
3M Scotchkote™ 445 Epoxy Slip Deterrent System Scotchkote Epoxy Slip Deterrent System 445 has been specifically developed as a 100% solids system for use with 3M Scotchkote Granular Aggregate to provide a slip deterrent finish to high risk floor.. |
|||
Thickness | 254 microns | 10.0 mil | Adhesive |
3M VHB™ F9473PC Adhesive Transfer Tapes with Adhesive 100MP 3M™ VHB™ Adhesive Transfer Tapes F9460PC, F9469PC and F9473PC utilize the 3M™ High Performance Acrylic Adhesive 100MP, which has excellent long term holding power with much higher adhesion streng.. |
|||
Thickness | 254 - 356 microns | 10.0 - 14.0 mil | |
3M 963-32 Flexible Prismatic Conspicuity Markings 3M Flexible Prismatic Conspicuity Markings Series 963 are highly retroreflective flexible microprismatic markings designed to mark the sides and rear of vehicles for enhanced visibility and detectio.. |
|||
Thickness | 254 microns | 10.0 mil | Overall Thickness |
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p.. |
|||
Thickness | 254 microns | 10.0 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin.. |