Thickness 200 - 1200 microns
7.87 - 47.2 mil
OCTAL DPET™ PET Sheet
Clear rigid sheet for use in general packaging; foam, fill, and seal; dairy products; and lamination. DPET™ sheet is produced directly from PET melt resin, resulting in enhanced optical and mechan..
Thickness >= 200 microns
>= 7.87 mil
Minimum Web
GrafTech GRAFCELL® FFP-200 SERIES Flow Field Plate Graphite
Manufactured from expanded natural graphite, GRAFCELL® Flow Field Plate (FFP) components retain a continuous graphitic phase. This phase continuity, combined with a low contact resistance, provid..
Thickness 200 - 3000 microns
7.87 - 118.1 mil
<1±0.03 :: 1-1.5±0.05 :: >1.5±0.6
Sinotek Materials B Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
Thickness 200 microns
7.87 mil
Shandong Dongyue Shenzhou New Material Co CHFM 200 Perfluorosulfonic Acid Proton Exchange Membrane (PFSAPEM)
Conformable with: Q/DYS 013-2007Perfluorosulfonic Acid Proton Exchange Membrane is a special polymer, mainly used for the processing of fuel cell membrane and chlor-alkali ion exchange membrane. Th..
Thickness 200 - 400 microns
7.87 - 15.7 mil
CeramTec Rubalit® HSS Alumina, 75% (High Strength Substrate)
Rubalit® HSS (High Strength Substrate) displays the successful union of elasticity and strength. The ultrafine microstructure of Rubalit® HSS is the basis for its outstanding substrate surface qua..
Thickness 200 - 240 microns
7.87 - 9.45 mil
AK Steel TRAN-COR® H-0 CARLITE® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Thickness 200 - 240 microns
7.87 - 9.45 mil
AK Steel TRAN-COR® H-0 CARLITE® DR® Grain Oriented Electrical Steel
TRAN-COR H CARLITE® high permeability electrical steels offer an outstanding degree of grain orientation, This combination of higher permeability with low residual stress offers the potential for l..
Thickness 200 - 3000 microns
7.87 - 118.1 mil
<1±0.03 :: 1-1.5±0.05 :: >1.5±0.5
Sinotek Materials A Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
Thickness 200 - 3000 microns
7.87 - 118.1 mil
<1±0.03 :: 1-1.5±0.05 :: >1.5±0.7
Sinotek Materials C Graphite Sheet
Flexible Graphite Sheet/Roll is made from expanding Expandable Graphite under high temperature and then rolling. It has the characteristics of high temperature resistance, corrosion resistance and g..
Thickness 200 - 1200 microns
7.87 - 47.2 mil
Average value: 404 microns Grade Count:8
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), Unreinforced". Each property range of values reported is minimum and m..
Copyright © lookpolymers.com All Rights Reserved