Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 2.00 - 6.00 microns | 0.0787 - 0.236 mil | General plating (excluding exotic metals) |
Parker Chomerics SPRING-LINE® Beryllium-Copper Gasket Description: SPRING-LINE beryllium-copper gaskets combine high levels of EMI shielding effectiveness with spring-finger wiping and low closure force properties. The high performance qualities of ber.. |
|||
Thickness | 2.00 - 10.0 microns | 0.0787 - 0.394 mil | |
Möller Medical TafSkin 109 L NanoCoating Electrically conducting, chemical-resistant, thin, easy-to-clean PTFE coatingInformation provided by Möller Medical, Member of CENTROTEC Group |
|||
Thickness | 2.00 - 6.00 microns | 0.0787 - 0.236 mil | |
Eifeler Coatings Technology CrCN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Thickness | 2.00 - 6.00 microns | 0.0787 - 0.236 mil | |
Eifeler Coatings Technology CrN PVD Coating Key Characteristics: low stress / good adhesion, high toughness and corrosion resistancePrimary Applications: drawing, pressing, bending and stamping of copper and other non-ferrous materials; metal.. |
|||
Thickness | 2.00 - 5.00 microns | 0.0787 - 0.197 mil | |
Eifeler Coatings Technology CROSAL® AlCrN PVD Coating This unique AlCrN based high performance coating has specially been developed for applications at high or highest temperatures.Information provided by Eifeler Coatings Technology |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® plus PVD Coating Key Characteristics: high hardness, very good oxidation resistance, low thermal conductivityPrimary Applications: machining of hardened steel and thicker steel sheets; excellent chemical resistance;.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® rose PVD Coating Key Characteristics: high hardness and elasticity, low friction, high oxidation resistancePrimary Applications: excellent for stainless steel and nickel-based high temperature alloys; hard and copy .. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology EXXTRAL® silver PVD Coating Key Characteristics: high hardness, good oxidation resistance, low frictionPrimary Applications: machining of abrasive or sticking materials (stainless steel, cast iron, Si-rich Al-alloys); machinin.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology SISTRAL® AlTiN PVD Coating Key Characteristics: extreme wear resistance at high temperature, excellent oxidation resistancePrimary Applications: excellent choice for cutting under extreme conditions (hard abrasive materials, .. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology SUPRAL TiAlN PVD Coating A TiAlN-based hard coating, especially developed for drilling under extreme conditions.Information provided by Eifeler Coatings Technology |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology TiCN PVD Coating Key Characteristics: high hardness excellent abrasive wear resistance, enhanced toughnessPrimary Applications: machining of difficult to machine alloy steels; high performance cutting where moderate.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology TiN PVD Coating Key Characteristics: standard all purpose coatingPrimary Applications: machining / cutting of iron based material; metal forming; plastic molding of highly abrasive plastics; orthopedic instrumentat.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology VARIANTA® TiAlN PVD Coating Key Characteristics: high hardness, very good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of cast iron and nickel base.. |
|||
Thickness | 2.00 - 4.00 microns | 0.0787 - 0.157 mil | |
Eifeler Coatings Technology VARIANTIC® TiAlCN PVD Coating Key Characteristics: low friction, good oxidation resistancePrimary Applications: coating for a wide range of carbide, cermet and high speed steel tools; machining of all types of steel under dry as.. |