Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 178 microns | 7.00 mil | Thermal Conductor Thickness |
Parker Chomerics T-Wing™ Heat Spreader Chomerics family of thin heat spreaders provides a low-cost, effective means of cooling IC devices in restricted spaces where conventional heat sinks are not appropriate. T-Wing spreaders consist of.. |
|||
Thickness | 178 - 1270 microns | 7.00 - 50.0 mil | |
Alcoa KAMA 4200 RPET
(discontinued **) CapabilitiesGauge: .007” to .050” (178 to 1270µm)Width: 12” to 48” (305 to 1219mm)Core size: 6” standard, 3” and 8” availableRoll O.D.: 29” standard, available up to 40”Up to 100% recycled.. |
|||
Thickness | 178 - 1520 microns | 7.00 - 60.0 mil | |
Alcoa KAMA 3300 Very High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Thickness | 178 - 1520 microns | 7.00 - 60.0 mil | |
Alcoa KAMA 3400 Super High Impact Polystyrene
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableMono-layer an.. |
|||
Thickness | 178 - 1520 microns | 7.00 - 60.0 mil | |
Alcoa KAMA AgriHIPS 3500 AgriHIPS
(discontinued **) CapabilitiesGauge: .007” to .060” (178 to 1524µm)Width: 12” to 62” (304 to 1575mm)Core Size: 6” standard cores, 3” and 8” availableRoll O.D.: 29” standard, up to 40” availableSilicone coat.. |
|||
Thickness | 178 microns | 7.00 mil | Nominal |
DuPont™ Nomex® 411 Paper, 7 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 48366X007 0.007" (0.178 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Thickness | >= 178 microns | >= 7.00 mil | Side 2 |
Arlon 55596R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 178 - 330 microns | 7.00 - 13.0 mil | Overall |
Arlon 910-07RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 178 - 254 microns | 7.00 - 10.0 mil | Overall |
Arlon 910-10RXX-P0 0.010" (0.254 mm) Self-Fusing Silicone Tape Design/Construction:Cross Section Type: RectangularArlon Rectangular Tape: Rectangular tape is of uniform thickness and is ideal for applications where a smooth, even layer of tape is not required.P.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37053W007 0.007" (0.178 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1 Interleave: Polyethylene Side 1: Cured Silicone Rubber Substrate: Style 2133 FiberglassSide 2: Cured Silicone RubberSide 2 Interleave: PolyethyleneThis data represents ty.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM015 Indoor UL Recognized Clear Polyester Overlaminate Label Product 3M™ Indoor UL Recognized Clear Polyester Overlaminate Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester overlami.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FM065 Indoor UL Recognized Brite Silver Polyester Label Products 3M™ Indoor UL Recognized Brite Silver Polyester Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These polyester labels utilize.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV365 Soft Yellow Vinyl Label Products 3M™ Soft Yellow Vinyl Label Products are flexible, conformable vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212, which is a high clar.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-72 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 - 203 microns | 7.00 - 8.00 mil | with adhesive |
3M Scotchlite™ 680CR-76 Removable Reflective Graphic Film with Comply™ Adhesive 7-mil, enclosed lens, retroreflective, engineered grade films that offer flexible and versatility; Available in 11 colors, including black (which reflects white); Similar daytime and nighttime appea.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 47571R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone Rubber Substrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene Appearance: Red silicone gum on fibergl.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7033 Screen Printable Polyester Performance LabelProducts 3M™ Screen Printable Polyester Performance Label Products are durable, high performance materials that offer excellent thermal stability and moisture resistance. These topcoated polyester label st.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M 7045 Screen Printable Vinyl Performance Label Products 3M™ Screen Printable Vinyl Performance Label Products 7045 and 7052 are durable, high performance materials that offer good durability and moisture resistance. These vinyl label stocks utilize 3M™.. |
|||
Thickness | 178 microns | 7.00 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 55638R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 2: Uncured Silicone Rubber Substrate: Style 162 Fiberglass Side 1: Cured Silicone Rubber Product Use: Flexible heater SubstrateAppearance: Red silic.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FP012605 White Polyester Label Products ion 3M™ White Polypropylene Label Products are glossy white opaque materials that offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1212, which is a hi.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FS025 Clear Polystyrene Label Products 3M™ Clear Polystyrene Label Products are hard, rigid film materials that offer economic alternatives for indoor applications. These polystyrene labels utilize 3M™ Adhesive P1212, which is a high c.. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV035 Indoor UL Recognized White Vinyl Label Products 3M™ Indoor UL Recognized White Vinyl Label Products are flexible, conformable white vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive P1212,.. |
|||
Thickness | 178 microns | 7.00 mil | |
3M Scotch® 35 Vinyl Electrical Tape Scotch® Vinyl Electrical Tape 35 is a 7 mil (0.178 mm) polyvinyl chloride (PVC) color-coding tape. Outstanding electrical and mechanical properties make this tape excellent for use in phase identif.. |
|||
Thickness | 178 microns | 7.00 mil | ASTM D1000 |
3M Temflex™ 1776 Vinyl Electrical Tape 3M™ Temflex™ Vinyl Electrical Tape 1776 is a good quality, economical, general-purpose vinyl insulating tape, manufactured in the USA. It has excellent resistance to abrasion, moisture, alkalies, .. |
|||
Thickness | 178 microns | 7.00 mil | Liner |
3M FV016405 Removable Vinyl Label Products 3M™ Removable Vinyl Label Products are flexible, conformable clear vinyl label stocks that offer durability and moisture resistance. These vinyl labels utilize 3M™ Adhesive R3500, which is designe.. |
|||
Thickness | >= 178 microns | >= 7.00 mil | |
Parker Chomerics CHO-BOND 1038 Conductive Silicone RTV Adhesive Electrically conductive, one component silicone adhesive/sealant that may be used for bonding EMI gaskets or for providing EMI and environmental protection as a caulk. This material cures on exposur.. |
|||
Thickness | 178 microns | 7.00 mil | Overall; Arlon SQA-TMS-003 |
Arlon 47581R007 0.007" (0.178 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: PESide 1: Uncured Silicone RubberSubstrate: 2113 Style FiberglassSide 2: Uncured Silicone RubberInterleave 2: PE This data represents typical values for the produc.. |