Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 145 microns | 5.70 mil | |
Hexcel® HexForce™ 1064 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 145 microns | 5.70 mil | ASTM D3652 |
3M Scotch® 8959 Bi-Directional Filament Tape Scotch® Filament Tape 8959 is a bi-directional specialty packaging tape reinforced with continuous glass yarns in both the longitudinal and transverse direction along with a biaxially oriented poly.. |
|||
Thickness | 145 microns | 5.70 mil | |
3M Scotch Pad™ 819 Filament Tape Pads 3M™ ScotchPad™ Filament Tape Pad 819 is a pre-cut pad formed with layered high performance filament tape sheets featuring biaxially oriented polypropylene backing with continuous glass yarns that .. |