Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 122 microns | 4.80 mil | 2 oz. Total Thickness; ASTM D1000 |
Parker Chomerics CHO-MASK II HT Conductive Foil Tape The CHO-MASK II family of EMI foil tapes includes both Standard Tack (ST) and High Tack (HT) versions for providing a conductive, non-corroding surface on painted metal electronic enclosures. CHO-MA.. |
|||
Thickness | 122 microns | 4.80 mil | Total Thickness |
3M 9832 Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |
|||
Thickness | 122 microns | 4.80 mil | ASTM D3652 |
3M Scotch® 215 Fine Line Tape Scotch® Fine Line Tape 215 is a very conformable film backed tape used to achieve excellent color separation on highly contoured surfaces.Information provided by 3M |
|||
Thickness | 122 microns | 4.80 mil | Total; ASTM D3752 |
3M 365 Thermosetable Glass Cloth Tape 3M™ Glass Cloth Tape 365 is a thermosetable rubber-resin adhesive tapes coated onto a strong conformable glass backing for many applications requiring high adhesion for adhesion to a variety of sur.. |
|||
Thickness | 122 microns | 4.80 mil | Total; ASTM D3752 |
3M 3650 Thermosetable Glass Cloth Tape 3M™ Glass Cloth Tape 3650 is a thermosetable rubber-resin adhesive tapes coated onto a strong conformable glass backing for many applications requiring high adhesion for adhesion to a variety of su.. |
|||
Thickness | 122 microns | 4.80 mil | Total Thickness |
3M 9832HL Double Coated Tapes with Adhesive 300MP 3M™ Double Coated Tape 9832 with Adhesive 300MP is a general purpose tape that provides excellent adhesion to a wide variety of substrates, including many foams, plastics, foil, and felt. This tape.. |