Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 1.80 - 3.60 microns | 0.0709 - 0.142 mil | |
Dow CYCLOTENE™ XU35132 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ XU35132 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |