Physical Properties | Metric | English | Comments |
---|---|---|---|
Pellet Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Trelleborg Fillite® 160W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Trelleborg Fillite® SGHA (500HA) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.700 - 0.900 g/cc | 0.0253 - 0.0325 lb/in³ | |
Trelleborg Fillite® 300W Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |