Physical Properties | Metric | English | Comments |
---|---|---|---|
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® 160 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® 52/7S (355) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® FG (300) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® 106 Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® SG (500) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |
|||
Pellet Density | 0.600 - 0.850 g/cc | 0.0217 - 0.0307 lb/in³ | |
Trelleborg Fillite® PG (300LF) Alumino-silicate Cenospheres Fillite is a glass hard, inert, hollow silicate sphere. Fillite is primarily used to reduce the weight of plastics, rubbers, resins, cement, etc., but also imparts further benefits in many situatio.. |