Polymer Property : Cell Length = 0.0177 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Cell Length 0.450 mm
0.0177 in
Typical Diameter
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..
Cell Length 0.450 mm
0.0177 in
Typical Diameter
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam
Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta..