Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | |
Zotefoams Evazote® EV30 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | |
Zotefoams Evazote® VA35 Ethylene Vinyl Acetate Copolymer Foam Evazote® is a closed cell, cross-linked EVA copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outsta.. |
|||
Cell Length | 0.300 mm | 0.0118 in | Typical Diameter |
Zotefoams Plastazote® LD24FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 mm | 0.0118 in | Typical Diameter |
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 - 0.700 mm | 0.0118 - 0.0276 in | |
Zotefoams Plastazote® LD24MC Low Density Polyethylene Foam, Medium Cell Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 - 0.600 mm | 0.0118 - 0.0236 in | |
Zotefoams Plastazote® LD30 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 mm | 0.0118 in | Typical Diameter |
Zotefoams Plastazote® LD30SD Static Dissipative Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 mm | 0.0118 in | Typical Diameter |
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.300 mm | 0.0118 in | Typical Diameter |
Zotefoams Supazote® EM26 Lightweight Supersoft Ethylene Copolymer Foam Supazote® is a closed cell, cross-linked copolymer foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outstandi.. |