Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.150 - 0.450 mm | 0.00591 - 0.0177 in | |
Zotefoams Plastazote® LD23 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.450 mm | 0.00591 - 0.0177 in | |
Zotefoams Plastazote® LD24FM Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.450 mm | 0.00591 - 0.0177 in | |
Zotefoams Plastazote® LD24FMSV Low Density Polyethylene Foam, Flame Retarded Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.450 mm | 0.00591 - 0.0177 in | |
Zotefoams Plastazote® LD24FR Low Density Polyethylene Foam, Flame Retardant Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.450 mm | 0.00591 - 0.0177 in | |
Zotefoams Plastazote® LD24 Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.500 mm | 0.00591 - 0.0197 in | |
Zotefoams Plastazote® MP33 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.500 mm | 0.00591 - 0.0197 in | |
Zotefoams Plastazote® MP34 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.150 - 0.500 mm | 0.00591 - 0.0197 in | |
Zotefoams Plastazote® MP45 Metallocene Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |