Physical Properties | Metric | English | Comments |
---|---|---|---|
Cell Length | 0.600 - 1.30 mm | 0.0236 - 0.0512 in | |
Zotefoams Plastazote® HL79 Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |
|||
Cell Length | 0.600 - 1.30 mm | 0.0236 - 0.0512 in | |
Zotefoams Plastazote® LD32CN Conductive Low Density Polyethylene Foam Plastazote® is a closed cell, cross-linked polyethylene foam manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and outs.. |