| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 25.1 g/10 min @Load 5.00 kg, Temperature 300 °C |
25.1 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
| SABIC Innovative Plastics NORYL EXNL0143 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||
| Melt Flow | 25.1 g/10 min @Load 5.00 kg, Temperature 300 °C |
25.1 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
| SABIC Innovative Plastics NORYL PX1736 PPE+PS Noryl PX1736 Resin is a blend of PPE and PS, that provides high strength, increased heat resistance, and translucency. The material has melt strenght suitable for Extrusion and Blow Molding applica.. |
|||