| Physical Properties | Metric | English | Comments |
|---|---|---|---|
| Melt Flow | 14.6 g/10 min @Load 10.0 kg, Temperature 250 °C |
14.6 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
| Samsung Cheil Industries Infino® FD-1112 PC, FR Information provided by Samsung Cheil Industries. |
|||