Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.00 - 58.8 g/10 min | 1.00 - 58.8 g/10 min | Average value: 15.7 g/10 min Grade Count:223 |
Overview of materials for Acetal Copolymer, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Acetal Copolymer, Unreinforced". Each property range of values reported is minimum and maximum values of.. |