Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 6.00 - 43.5 g/10 min | 6.00 - 43.5 g/10 min | Average value: 26.2 g/10 min Grade Count:3 |
Overview of materials for Polyethersulfone (PES), 20% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 20% Glass Fiber Filled". Each property range of values reported is minimum and m.. |