Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 1.0 - 4.0 g/10 min | 1.0 - 4.0 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE A 6900 LC BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 3.0 - 4.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 - 4.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PC-GP1-[color]-LF Polycarbonate, General Purpose, Food Contact Polycarbonate, General Purpose, Low FlowFeatures: • Food Contact AcceptableProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, .. |
|||
Melt Flow | 1.0 - 4.0 g/10 min @Load 3.80 kg, Temperature 300 °C |
1.0 - 4.0 g/10 min @Load 8.38 lb, Temperature 572 °F |
ASTM D1238 |
Polymer Resources PPX/NY G20 PPO/Nylon 66 Alloy , 20% Glass Reinforced Polyphenylene Oxide/Nylon 66 Alloy , 20% Glass ReinforcedProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informa.. |
|||
Melt Flow | 0.10 - 4.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
0.10 - 4.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-GP6 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 290F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Flow | 0.10 - 4.0 g/10 min @Load 11.6 kg, Temperature 250 °C |
0.10 - 4.0 g/10 min @Load 25.6 lb, Temperature 482 °F |
ASTM D1238 |
Polymer Resources PPX-GP7 Modified-PPO, General Purpose Modified-Polyphenylene Oxide, General Purpose, 300F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Informati.. |
|||
Melt Flow | 2.0 - 4.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
2.0 - 4.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1010G40 HB Polycarbonate, 40% Fiberglass Reinforced Information provided by Ravago. |
|||
Melt Flow | 1.0 - 4.0 g/10 min | 1.0 - 4.0 g/10 min | ASTM D1238 |
Polymer Resources PPX/NY G20 Modified PPO, 20% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 2.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
2.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Bio-Flex® F 1110 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Melt Flow | 3.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
FKuR Kunststoff Terralene® WF 6534 Biobased Polyethylene With the brand name Terralene® FKuR offers biobased polyethylene compounds made using Braskem's Green PE. When compared to conventional polyethylene (PE), the main difference is that the ethanol.. |
|||
Melt Flow | 3.0 - 4.0 g/10 min | 3.0 - 4.0 g/10 min | ASTM D1238 |
Micropol Microlin ML20 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Melt Flow | 3.0 - 4.0 g/10 min | 3.0 - 4.0 g/10 min | ASTM D1238 |
Micropol Microlin ML25 Linear Polyethylene Rotational Molding Powder Information provided by Micropol Limited |
|||
Melt Flow | 2.0 - 4.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
2.0 - 4.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
nominal; ASTM D1238 |
MRC Polymers SATRANâ„¢ 800R ABS Terpolymer, Reprocessed black onlyInformation provided by MRC Polymers Inc. |
|||
Melt Flow | 2.1 - 4.0 g/10 min | 2.1 - 4.0 g/10 min | |
Shandong Dongyue Shenzhou New Material Co DS601 Perfluorinated Ethylene-Propylene Copolymer Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene resin is the copolymer of the TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and.. |
|||
Melt Flow | 2.5 - 4.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
2.5 - 4.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Features: Copolymer; High ViscosityUses: PipingAdditional Properties: Crystallization Heat - ASTM .. |
|||
Melt Flow | 2.0 - 4.0 g/10 min | 2.0 - 4.0 g/10 min | ASTM D1238 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Melt Flow | 2.0 - 4.0 g/10 min | 2.0 - 4.0 g/10 min | ASTM D1238 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Melt Flow | 2.0 - 4.0 g/10 min | 2.0 - 4.0 g/10 min | ASTM D1238 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Melt Flow | 2.0 - 4.0 g/10 min | 2.0 - 4.0 g/10 min | ASTM D1238 |
A. Schulman PP 1188-01 Polypropylene Extra High-Impact Polypropylene DescriptionPolypropylene PP 1188-01 is an extra high-impact polypropylene, copolymer type, with excellent low temperature properties. Information provided by A. Schulman. |
|||
Melt Flow | 1.0 - 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
1.0 - 4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Cossa Polimeri ESTAPROP H0260 MC/EC Conductive Polypropylene, Mineral Filled Information provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 2.0 - 4.0 g/10 min @Load 5.00 kg, Temperature 232 °C |
2.0 - 4.0 g/10 min @Load 11.0 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 6000 HD Polyvinylidene Fluoride - Injection Molding Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili.. |
|||
Melt Flow | 2.5 - 4.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
2.5 - 4.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 60512 Polyvinylidene Fluoride (PVDF)
(Unverified Data**) Solef® 60512 PVDF copolymer has high viscosity of the melt and it is a grade for offshore piping.Information provided by Solvay Specialty Polymers. |
|||
Melt Flow | 1.0 - 4.0 g/10 min | 1.0 - 4.0 g/10 min | ASTM D1238 |
Polymer Resources PPX/NY G30 Modified PPO, 30% Glass Reinforced PPX/Nylon 6,6 Alloy
(Unverified Data**)&l Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 1.0 - 4.0 g/10 min | 1.0 - 4.0 g/10 min | ASTM D1238 |
Polymer Resources PPX-G30 Modified PPO, 30% Glass Reinforced
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |
|||
Melt Flow | 0.10 - 4.0 g/10 min | 0.10 - 4.0 g/10 min | ASTM D1238 |
Polymer Resources PPX-GP7 Modified PPO, General Purpose with HDT of 300 F
(Unverified Data**) Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Information provided by Polymer Resources Corporation. |