Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 5.00 - 39.3 g/10 min | 5.00 - 39.3 g/10 min | Average value: 31.5 g/10 min Grade Count:9 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |