Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 22 - 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
22 - 28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238/L |
NIZHNEKAMSKNEFTEKHIM PP 4340R (EP2Z29G) Propylene and Ethylene Copolymer Product obtained by copolymerization of propylene with ethylene in presence of complex metalorganic catalysts. It incorporates increased long-term thermal stability, thermal-oxidative degradation r.. |
|||
Melt Flow | 22 - 28 g/10 min @Load 3.80 kg, Temperature 230 °C |
22 - 28 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Ravago Manufacturing Americas Hylex® P1025G10 HB Polycarbonate, 10% Glass Reinforced Information provided by Ravago. |
|||
Melt Flow | 14 - 28 g/10 min @Load 5.00 kg, Temperature 230 °C |
14 - 28 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id.. |
|||
Melt Flow | 14 - 28 g/10 min @Load 5.00 kg, Temperature 230 °C |
14 - 28 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kraton® FG1901 G (SEBS) Linear Block Copolymer Description: Kraton FG1901 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 30%. It is supplied from North America in the physical form id.. |
|||
Melt Flow | 14 - 28 g/10 min @Load 5.00 kg, Temperature 230 °C |
14 - 28 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Kraton® FG1901 G (SEBS) grafted with MA Description: Kraton FG1924 G is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 13% . It is supplied from North America in the physical form i.. |
|||
Melt Flow | 22 - 28 g/10 min @Load 5.00 kg, Temperature 372 °C |
22 - 28 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P455 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melt Flow | 20 - 28 g/10 min @Load 5.00 kg, Temperature 365 °C |
20 - 28 g/10 min @Load 11.0 lb, Temperature 689 °F |
ASTM D1238 |
Solvay Specialty Polymers Radel® R-5800 Polyphenylsulfone (PPSU) Radel® R-5800 is a high melt flow grade of Radel® polyphenylsulfone (PPSU). It is especially well-suited for parts requiring long flow length with thin walls. Radel® resins offer exceptiona.. |
|||
Melt Flow | 24 - 28 g/10 min @Load 2.16 kg, Temperature 230 °C |
24 - 28 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Samyang Triel® 5301SP Thermoplastics Polyetherester Elastomer, Double Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5301SP is intended for double extrusion.Information provided by Samyang. |
|||
Melt Flow | 22 - 28 g/10 min @Load 5.00 kg, Temperature 372 °C |
22 - 28 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® MFA® 1041 Perfluoropolymer Hyflon® MFA 1041 is a high extrusion speed resin specifically designed for insulation for plenum-rated LAN cables. MFA 1041 delivers superior electrical performance in addition to its excellent f.. |
|||
Melt Flow | 22 - 28 g/10 min @Load 3.80 kg, Temperature 230 °C |
22 - 28 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238 |
Entec Hylex® P1025G10NHFR Polycarbonate, 10% Glass Reinforced Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Melt Flow | 18 - 28 g/10 min | 18 - 28 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1110 PBT Can be used directly for spinning, or it can be used after reinforcement & compounding. It can also be used to produce cable sheath through tackificationInformation provided by Beijing Ranger Chemic.. |
|||
Melt Flow | 7.0 - 28 g/10 min @Load 12.5 kg, Temperature 232 °C |
7.0 - 28 g/10 min @Load 27.6 lb, Temperature 450 °F |
ASTM D1238 |
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha.. |
|||
Melt Flow | 25 - 28 g/10 min | 25 - 28 g/10 min | |
Ashley Polymers Ashlene® R195B Acetal A general purpose, low viscosity with excellent toughness, strength, stiffness, lubricity in black. Available in UV stabilized grades: R195-B2 (good weatherability); R195-HB2 (maximum weatherabili.. |
|||
Melt Flow | 24.1 - 28 g/10 min | 24.1 - 28 g/10 min | C |
Shandong Dongyue Shenzhou New Material Co DS608 Fluorinated Ethylene-Propylene Copolymer For High-Speed Extrusion Conformable with: Q/DYS 003-2007Fluorinated Ethylene Propylene is the copolymer of TFE and HFP, with good thermal stability, outstanding chemical inertness, good electrical insulation, and low coeff.. |