Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 200 g/10 min | 3.00 - 200 g/10 min | Average value: 21.5 g/10 min Grade Count:22 |
Overview of materials for EMAAA Terpolymer This property data is a summary of similar materials in the MatWeb database for the category "EMAAA Terpolymer". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melt Flow | 150 - 200 g/10 min @Load 2.16 kg, Temperature 170 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® DIPP-539 Linear Thermoplastic Polyurethane
(discontinued **) PEARLBOND® DIPP-539 is a linear, polycaprolactone-copolester polyurethane with a very high crystallization rate and a very high thermoplasticity level.Applications: PEARLBOND® DIPP-539 can be adde.. |
|||
Melt Flow | 0.400 - 200 g/10 min | 0.400 - 200 g/10 min | Average value: 32.4 g/10 min Grade Count:8 |
Overview of materials for Polybutene This property data is a summary of similar materials in the MatWeb database for the category "Polybutene". Each property range of values reported is minimum and maximum values of appropriate MatWeb .. |
|||
Melt Flow | 150 - 200 g/10 min @Load 2.16 kg, Temperature 170 °C |
150 - 200 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials Pearlbond® 539 Thermoplastic Polyurethane Pearlbond® 539 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level.Appl.. |