Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.00 - 20.0 g/10 min | 3.00 - 20.0 g/10 min | Average value: 8.50 g/10 min Grade Count:4 |
Overview of materials for Nylon 6, 20% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ.. |
|||
Melt Flow | 1.00 - 20.0 g/10 min @Load 21.6 kg, Temperature 190 °C |
1.00 - 20.0 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB1411 Linear Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 - 20.0 g/10 min @Load 21.6 kg, Temperature 200 °C |
4.00 - 20.0 g/10 min @Load 47.6 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2185 High Impact Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (300000 ppm) Forms: Pellets Features: General PurposeInformation Provided by Teknor Apex |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW2878 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (600000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW2888 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW3422 Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (700000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 1.10 - 20.0 g/10 min | 1.10 - 20.0 g/10 min | Average value: 5.68 g/10 min Grade Count:16 |
Overview of materials for Thermoplastic Olefinic Elastomer (TPO), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Olefinic Elastomer (TPO), Film Grade". Each property range of values reported is minimum a.. |
|||
Melt Flow | 0.700 - 20.0 g/10 min | 0.700 - 20.0 g/10 min | Average value: 2.83 g/10 min Grade Count:46 |
Overview of materials for Ionomer, Molded This property data is a summary of similar materials in the MatWeb database for the category "Ionomer, Molded". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
Melt Flow | 1.00 - 20.0 g/10 min | 1.00 - 20.0 g/10 min | Average value: 10.8 g/10 min Grade Count:9 |
Overview of materials for Polyphenylene Ether, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Ether, 20% Glass Filled". Specific grades with glass content between 15% and 24% are inclu.. |
|||
Melt Flow | 6.00 - 20.0 g/10 min | 6.00 - 20.0 g/10 min | Average value: 12.1 g/10 min Grade Count:4 |
Overview of materials for Polyethylene Terephthalate (PET), 40% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 40% Glass Reinforced". Specific grades with glass content between 35% .. |
|||
Melt Flow | 5.00 - 20.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
5.00 - 20.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBW011LE Low Density Polyethylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Titanium Dioxide (TiO2) (400000 ppm) Features: General Purpose Forms: PelletsInformation Provided by Teknor.. |
|||
Melt Flow | 3.00 - 20.0 g/10 min | 3.00 - 20.0 g/10 min | Average value: 9.28 g/10 min Grade Count:90 |
Overview of materials for Polystyrene, Flame Retardant This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Flame Retardant". Each property range of values reported is minimum and maximum values of a.. |
|||
Melt Flow | 3.00 - 20.0 g/10 min | 3.00 - 20.0 g/10 min | Average value: 12.8 g/10 min Grade Count:13 |
Overview of materials for Polypropylene with 10% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 10% Mica Filler". Specific grades with primary filler content between 5% and 14% are .. |
|||
Melt Flow | 4.00 - 20.0 g/10 min | 4.00 - 20.0 g/10 min | Average value: 11.1 g/10 min Grade Count:16 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |