Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in antist.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® MFA® P6010 Perfluoropolymer Hyflon® MFA P6010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® MFA® P6310 Perfluoropolymer Hyflon® MFA P6310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA) Hyflon® PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat res.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P7310 Perfluoroalkoxy (PFA) Hyflon® PFA P7310 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melt Flow | 12 - 17 g/10 min @Load 5.00 kg, Temperature 365 °C |
12 - 17 g/10 min @Load 11.0 lb, Temperature 689 °F |
ASTM D1238 |
Solvay Specialty Polymers Radel® R-5500 Polyphenylsulfone (PPSU) Radel® R-5500 is a general purpose extrusion grade of polyphenylsulfone (PPSU), offering exceptional hydrolytic stability and better toughness than most commercially available high-temperature po.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P7010 Perfluoroalkoxy (PFA) Hyflon® PFA P7010 is a clear, semi-crystalline melt processable perfluorinated resin. It is designed for electrostatic powder coatings and is particularly recommended for use as a topcoat in anti.. |
|||
Melt Flow | 11 - 17 g/10 min @Load 2.16 kg, Temperature 280 °C |
11 - 17 g/10 min @Load 4.76 lb, Temperature 536 °F |
|
Zeon Chemicals Zeonor® 1060R Cyclo-Olefin Polymer Zeonor 1020R shall be in the form of pellets. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
|
Daikin NEOFLON AP-221SH PFA Semiconductor Grade NEOFLON PFA semiconductor grade.Applications: Linings, tubing, etc.Information provided by Daikin Industries. |
|||
Melt Flow | 15 - 17 g/10 min | 15 - 17 g/10 min | Cond. 300/1.2 |
Ashley Polymers Ashlene® 1021 Polycarbonate A general purpose injection molding grade, natural resin. Also available as: 1021R (with release), 1023 (with UV stabilizers); 1023R (with release and UV stabilizers).Data provided by the manufactu.. |
|||
Melt Flow | 15 - 17 g/10 min | 15 - 17 g/10 min | |
Ashley Polymers Ashlene® 1105 Polycarbonate, 5-7% Glass Reinforced A general purpose foamable injection molding grade resin with 5-7% glass reinforcement.Data provided by the manufacturer |
|||
Melt Flow | 15 - 17 g/10 min @Load 1.20 kg, Temperature 300 °C |
15 - 17 g/10 min @Load 2.65 lb, Temperature 572 °F |
Cond. O |
Ashley Polymers Ashlene® 1621 Polycarbonate A general purpose injection molding grade, natural resin, UL approved. Also available as: 1621R (with release); 1623 (with UV stabilizers); 1623R (with release and UV stabilizers).Data provided by .. |
|||
Melt Flow | 15 - 17 g/10 min | 15 - 17 g/10 min | Cond. O |
Ashley Polymers Ashlene® C1176 Polycarbonate These are also available with UV, designated by -3. For release, add R. These are all flame retardant grades developed for various applications such as electrical, electronic, lighting, computer, .. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA M640 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melt Flow | 10 - 17 g/10 min @Load 5.00 kg, Temperature 372 °C |
10 - 17 g/10 min @Load 11.0 lb, Temperature 702 °F |
ASTM D1238 |
Solvay Specialty Polymers Hyflon® PFA P450 Perfluoroalkoxy (PFA)
(Unverified Data**) Hyflon PFA is a unique family of semi-crystalline, melt processable perfluoropolymers which combine excellent mechanical characteristics to unique properties such as chemical inertness, heat resista.. |
|||
Melt Flow | 15 - 17 g/10 min | 15 - 17 g/10 min | Cond. 300/1.2 |
Ashley Polymers Ashlene® P1021R Polycarbonate A prime general purpose injection molding grade, natural resin with easy mold release.Data provided by the manufacturer |