Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 2.00 - 148 g/10 min | 2.00 - 148 g/10 min | Average value: 44.6 g/10 min Grade Count:34 |
Overview of materials for Nylon 66, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Unreinforced". Each property range of values reported is minimum and maximum values of appropr.. |