Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 90 - 145 g/10 min @Load 2.16 kg, Temperature 170 °C |
90 - 145 g/10 min @Load 4.76 lb, Temperature 338 °F |
DIN 53.735 |
Lubrizol Advanced Materials PEARLBOND® 102 Linear Thermoplastic Polyurethane PEARLBOND® 102 is a linear, polycaprolactone-based polyurethane, supplied in form of small white pellets, which combines a very high crystallization rate with a very high thermoplasticity level.A.. |
|||
Melt Flow | 90 - 145 g/10 min @Load 2.16 kg, Temperature 170 °C |
90 - 145 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 502 Linear Thermoplastic Polyurethane PEARLBOND™ 502 is a linear, polycaprolactone-copolyester polyurethane with a high crystallization rate and a very high thermoplasticity level.Application: Pearlbond™ 502 can be added to fo.. |