Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 0.770 - 13.0 g/10 min | 0.770 - 13.0 g/10 min | Average value: 3.05 g/10 min Grade Count:23 |
Overview of materials for Very Low Density Polyethylene (VLDPE) This property data is a summary of similar materials in the MatWeb database for the category "Very Low Density Polyethylene (VLDPE)". Each property range of values reported is minimum and maximum va.. |
|||
Melt Flow | 6.00 - 13.0 g/10 min | 6.00 - 13.0 g/10 min | Average value: 8.80 g/10 min Grade Count:5 |
Overview of materials for Acetal Homopolymer, PTFE-Filled This property data is a summary of similar materials in the MatWeb database for the category "Acetal Homopolymer, PTFE-Filled". Each property range of values reported is minimum and maximum values o.. |