Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 9.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
SABIC Innovative Plastics GELOY FXW749SK ASA Sparkle VisualFx ASA Resin - Weatherable |
|||
Melt Flow | 9.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and up to 25% post consumer recycle content. Availability of resin is restricted and lead times are.. |
|||
Melt Flow | 9.2 g/10 min @Load 1.20 kg, Temperature 300 °C |
9.2 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL8414 PC Copolymer (Asia Pacific) Lexan* EXL8414 is a PC/siloxane copolymer resin with medium flow, excellent low temperature impact and 25% post consumer recycle content. Limited availability and restricted color only. Higher color.. |
|||
Melt Flow | 9.2 g/10 min @Load 10.0 kg, Temperature 230 °C |
9.2 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM-D1238 |
Ineos ABS Lustran® LK197 ABS, Extrusion Grade Lustran® ABS LK197 resin is a high-gloss, medium-impact extrusion grade of ABS (Acrylonitrile Butadiene Styrene). It provides a superior balance between rigidity and impact strength, as well as e.. |
|||
Melt Flow | 9.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL HN731A PPE+PS PPE+PS blend. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant (restrictions apply). Combine.. |
|||
Melt Flow | 9.2 g/10 min @Load 5.00 kg, Temperature 280 °C |
9.2 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL 731 PPE+PS PPE+PS blend. Unfilled. NSF listed for potable water use in several colors (Standard 61). FDA compliant in several colors (restrictions apply). UL94 HB rated. Low water absorption. Hydrolytic stabi.. |
|||
Melt Flow | 9.2 g/10 min @Load 5.00 kg, Temperature 200 °C |
9.2 g/10 min @Load 11.0 lb, Temperature 392 °F |
Procedure A Condition G; ASTM D1238 |
Diamond Polymers ASA M-523 Description: ASA Weatherable Polymer, Injection Molding Grade, High HeatInformation provided by Diamond Polymers, Inc. |
|||
Melt Flow | 9.2 g/10 min @Load 10.0 kg, Temperature 220 °C |
9.2 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
Diamond Polymers DIAMALOY GLY FXW749 Sheet Extrusion Grade, Sparkle/Pearlescence Diamaloy GLY FXW749SK resin is a low impact grade of ASA (acrylonitrile-styrene-acrylate) with good resistance to weather aging and added visual effects (pearlescence). It has good melt strength for.. |