Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 1508 M Polypropylene Mica Filled, 15% by weight.Features:Rigidity, HighImpact Resistance, GoodForms:PelletsProcessing Methods:Injection MoldingUses:Automotive ApplicationsInformation provided by Multibase |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® HD-2007-H HDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability, very high melt strength.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provid.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
|
Polimeri Europa Dutral® OCP 2530 PL Ethylene - Propylene Dutral® OCP 2530 PL is an Ethylene - Propylene polymer produced by suspension polymerization using a Ziegler-Natta Catalyst. A non-staining antioxidant is added during the production process.Key F.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ASTM D1238 |
SABIC Innovative Plastics Cycoloy® C1150E PC+ABS (Asia Pacific) High impact, extrusion grade polycarbonate/ABS alloy. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® 3412HF PC 20% glass reinforced, high flow PC. UL rated V-1 at 0.059"", |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
LyondellBasell Lupolen® 5031 L HDPE, Injection Molding Grade Easy flow, injection molding grade for closures, aerosol pumps, spray nozzles for spray cans, small automotive parts such as the caps on lead/acid batteries, knobs, barrels for writing instruments a.. |
|||
Melt Flow | 8.5 - 11.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 - 11.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Kazanorgsintez PC-010 Polycarbonate Production Method: Obtained by means of polycondensation method. Application: Intended for product manufacture by method of die-casting.Information Provided by Kazanorgsintez |
|||
Melt Flow | 8.5 - 11 g/10 min | 8.5 - 11 g/10 min | ASTM D1238 |
Kolon KOCETAL® MS301 Wear Modified Acetal Resin Molybdenum disulfide added, improved wear property. Applications: Products for low noise and friction against metal. Information provided by API-Kolon. |
|||
Melt Flow | 8.5 - 19 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 - 19 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Kraton® D1161 B (SIS) Linear Block Copolymer Description: Kraton D1161 B is a clear, linear block copolymer based on styrene and isoprene with a polystyrene content of 15%. It is supplied from South America in the physical form identified: Kra.. |
|||
Melt Flow | 8.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
8.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics LNP LUBRICOMP DX98306H PC (Asia Pacific) LNP* Lubricomp* DX98306H is a compound based on Polycarbonate resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated, Low Extractible. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL SE1X PPE+PS PPE+PS blend. Unfilled. Non-brominated, non-chlorinated FR system. UL94 V1, UL746C F1. Dielectric strength. Suitable for E/E market indoor/outdoor applications. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 Conductive GTX, CTE 7 |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX987 PPE+PA66 (Asia Pacific) Conductive GTX, CTE 7 |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 250 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL NWP100 PPE+HIPS (Asia Pacific) PPO/HIPS Unfilled high impact extrusion grade |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ISO 1133 |
Wico Plast Wicolon 807 Polycarbonate, U.V. Stabilized ApplicationsInjection moldingCharacteristics:U.V. stabilizedAll information provided by Wico Plast, Warenhandelsges. mbH |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Total PPH 3576 BB Polypropylene Homopolymer, Cast Film Polypropylene 3576 BB is recommended for use in non-oriented cast films processes. It contains an optimized level of slip and anti-block additives.3576 BB is intended for food, magazine or textile .. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Total PPH 3576 H Polypropylene Homopolymer, Cast Film Polypropylene 3576 H is recommended for use core layer in non-oriented cast films processes for the manufacture of packaging film with outstanding optical properties. 3576 H is specially designed f.. |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 200 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSC 536 Polystyrene Polystyrene 536 is a high melt flow; high heat crystal polystyrene. Designed for fast cycle injection molding and for high output, direct injection profile extrusion for foam applications.Informatio.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 706.15 Cast Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for coextruded cast film applications.Availability: Latin America, North America and South Ame.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene™ LD 706.15 Molding Ethylene Vinyl Acetate Copolymer Product Description: Escorene Ultra LD 706.15 is a 14.9 wt% vinyl acetate copolymer film resin designed for specialty molding, extrusion and compounding applications.Availability: Latin America, Nor.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
|
Chi Mei Kibiton® PB-5502 Styrene-Butadiene Copolymer Hot melt adhesive |
|||
Melt Flow | 8.5 g/10 min @Load 10.0 kg, Temperature 220 °C |
8.5 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polyrex® PG-33 Polystyrene Standard grade |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem PRA 0852 RACO Random Polypropylene Copolymer PRA 0852 is a medium melt flow rate random copolymer with slip and antiblocking agents. It is suitable for blown and cast film extrusion. PRA 0852 has excellent optical properties and good processab.. |
|||
Melt Flow | 8.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
8.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Azoty Tarnow™ TARNOFORM 300 K POM Tribological modified grade with addition of special chalk, which causes decrease of wear.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Melt Flow | 8.5 g/10 min | 8.5 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-15FG-1734 15% Glass Fiber Reinforced, Heat Stabilized Information provided by Asahi Thermofil |
|||
Melt Flow | 8.5 g/10 min @Load 5.00 kg, Temperature 260 °C |
8.5 g/10 min @Load 11.0 lb, Temperature 500 °F |
ISO 1133 |
Ineos ABS Triax® KU2-3154 ABS + Polyamide Blend (DAM), Injection Molding Grade Triax® KU2-3154 is mineral reinforced, easy-flowing, injection molding grade, and comes in pellets. It has reduced moisture absorption and very low warpage. |