Melt Flow 78 g/10 min

@Pressure 0.655 MPa
78 g/10 min

@Pressure 95.0 psi
Severs Efflux; Geon® ALTC 23 (with provided formulation); Internal Method
PolyOne Geon™ 180 Series 180X5 Polyvinyl Chloride Homopolymer (PVC Homopolymer)
Geon® 180X5 is low molecular weight resin that provides good chemical foam characteristics with excellent overblow resistence. The modified rheology of Geon® 180X5 provides increased viscosity and..
Melt Flow 78 g/10 min

@Load 2.16 kg,
Temperature 260 °C
78 g/10 min

@Load 4.76 lb,
Temperature 500 °F
Estimated using room temperature density; ISO 1133
Lanxess Pocan® KU 1-7301 000000 PBT
PBT, non-reinforced, injection molding, food contact
Melt Flow 78 g/10 min

@Load 10.0 kg,
Temperature 230 °C
78 g/10 min

@Load 22.0 lb,
Temperature 446 °F
Stellarchem SV-B40D TPV Compound
This grade of Stellarchem SV series is a dynamic crosslinked, EPDM/PP compound. It's design to replace thermoset elastomers, such as EPDM, and traditional Thermoplastic TPVs. It can be process on ..