Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 230 °C |
75 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CR750CL-02 Polypropylene, Random Copolymer, NX-8000 based COPYLENE™ CR750CL-02 is an easy molding, high melt flow random copolymer that has good see-through and contact clarity in injection molding applications and is formulated with advanced technology. .. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 230 °C |
75 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CR750CLS Polypropylene Random Copolymer Description: COPYLENE® CR750CLS is a clarified random copolymer specially designed and formulated for clear injection molding applications and is formulated with antistat and lube for excellent mol.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 380 °C |
75 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU)
(Unverified Data**) Veradel® PESU was formerly marketed as Gafone™ PESU Veradel 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughn.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 190 °C |
75 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Chevron Phillips HiD® 9075 HDPE Injection Molding Resin
(discontinued **) Resin Type: linear copolymer; ASTM D3350 Classification 335540A; ASTM D4976 Classification: PE 235, A 54607Characteristics: excellent flow, moderate impact strength, good stiffness, moderate ESCR, e.. |
|||
Melt Flow | 75 g/10 min @Load 5.00 kg, Temperature 316 °C |
75 g/10 min @Load 11.0 lb, Temperature 600 °F |
ASTM D1283 |
Chevron Phillips Ryton® P-4 Polyphenylene Sulfide Resin
(discontinued **) Characteristics: Excellent thermal stabilityExcellent chemical resistanceApplications: CoatingsCompoundsExtrusionInformation provided by Chevron Phillips.Solvay Specialty Polymers has acquired the R.. |
|||
Melt Flow | 75 g/10 min @Load 5.00 kg, Temperature 316 °C |
75 g/10 min @Load 11.0 lb, Temperature 601 °F |
Procedure B; ASTM D1283 |
Chevron Phillips Ryton® P-4-60 Polyphenylene Sulfide Resin
(discontinued **) Tan Color Polyphenylene Sulfide ResinRyton® P-4-60 is supplied as pellets. The powder form is P-4. Ryton® PPS exhibits excellent thermal stability and chemical resistance and is suitable for a v.. |
|||
Melt Flow | 75 g/10 min @Load 5.00 kg, Temperature 270 °C |
75 g/10 min @Load 11.0 lb, Temperature 518 °F |
Calculated from MVR using melt density; ISO 1133 |
Lanxess Durethan® A 30 S 000000 Nylon 66 PA 66 standard injection molding-grade, non-reinforced, good demolding, very rapid solidificationApplication Examples: plug connectors, terminal blocks, cable clips, bobbins |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 230 °C |
75 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® TEA 4001-35 Natural TPO Thermoplastic Polyolefin Elastomer Forms: PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 380 °C |
75 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® 3600 Polyethersulfone (PESU) Veradel® 3600 polyethersulfone (PESU) is a very high melt flow, transparent grade that offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to s.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 380 °C |
75 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU) Veradel® polyethersulfone (PESU) is transparent and offers high heat deflection temperatures, excellent toughness and dimensional stability, and resistance to steam, boiling water and mineral aci.. |
|||
Melt Flow | 75 g/10 min @Load 10.0 kg, Temperature 250 °C |
75 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 75 g/10 min @Load 5.00 kg, Temperature 250 °C |
75 g/10 min @Load 11.0 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500GN15 Polybutylene Terephthalate, 15% Glass Reinforced, Flame Retardant Characteristics:G/F reinforcedFlame retardantHeat and Impact resistantApplications:AutomotiveConnectorGearOutdoor handleIgnition systemElectronicConnectorGas valveCoil bobbinSwitch caseRelay caseO/A.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 190 °C |
75 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex MONPRENE® MP 2820M Thermoplastic Elastomer Information provided by Teknor Apex Company |
|||
Melt Flow | 75 g/10 min @Load 10.0 kg, Temperature 250 °C |
75 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® TN-1100 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 75 g/10 min @Temperature 230 °C |
75 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 2575N injection Molded Polypropylene Impact Copolymer for High Speed injection Molded ApplicationsFormolene® 2575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging, .. |
|||
Melt Flow | 75 g/10 min @Temperature 230 °C |
75 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6575N Impact Copolymer Polypropylene Impact Copolymer for High Speed injection Molded Applications Formolene® 6575N is a very high melt flow, medium impact copolymer of polypropylene. It is designed for such applications as packaging,.. |
|||
Melt Flow | 75 g/10 min | 75 g/10 min | ASTM D1238 |
Total PPC 5946WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 5946WZ is a nucleated impact copolymer with a Melt Flow index of 75 g/10 min.TOTAL Polypropylene 5946WZ is characterized by very low warpage, improved stiffness, a.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 230 °C |
75 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP7085E1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow, excellent stiffness/toughness balance and antistatic properties for good molding behavior. It is suitable for molding applica.. |
|||
Melt Flow | 75 g/10 min @Load 10.0 kg, Temperature 220 °C |
75 g/10 min @Load 22.0 lb, Temperature 428 °F |
Melt Volume Rate (ml/10 min); ISO 1133 |
Chi Mei Polylac® PA-756H ABS - High Flow Super high flow |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 190 °C |
75 g/10 min @Load 4.76 lb, Temperature 374 °F |
"E"; ASTM D1238 |
Aaron Industries AAROPRENE® ATPR 1000 70A Elastomeric Compound AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified. |
|||
Melt Flow | 75 g/10 min @Temperature 230 °C |
75 g/10 min @Temperature 446 °F |
I<sub>2</sub>; ASTM D1238 |
Formosa Plastics Formolene® 6375N Impact Copolymer Polypropylene Impact Copolymer For High Speed Injection Molded Applications Formolene® 6375N is a very high melt flow, low impact copolymer of polypropylene. It is designed for such applications as packaging, ho.. |
|||
Melt Flow | 75 g/10 min @Load 2.16 kg, Temperature 380 °C |
75 g/10 min @Load 4.76 lb, Temperature 716 °F |
ASTM D1238 |
Solvay Specialty Polymers Veradel® A-702 Polyethersulfone (PESU)