Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 65.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
65.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1736R Thermoplastic Elastomer Notes: Soft Material; Overmold onto PP handlesInformation Provided by Teknor Apex |