Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 230 °C |
60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
NCMT NanoPAC™ HS401 High Performance Polypropylene Nanocomposite Applications: Electrical AppliancesInformation provided by Nano Composite Materials Technology Limited |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 230 °C |
60 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP562T Fiber (Spunbond) Grade Polypropylene Moplen HP562T is the controlled rheology polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP562T is a homopolymer particularly suitable f.. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 230 °C |
60 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HP740T Injection Molding (Thin Wall) Grade Polypropylene Moplen HP740T is a nucleated polypropylene HOMO polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP740T is a homopolymer selected by customers for use in t.. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 240 °C |
60 g/10 min @Load 4.76 lb, Temperature 464 °F |
ASTM D1238 |
Shell Carilon® D26VM100 Polyketone, High-Flow Injection Molding Grade
(discontinued **) Shell announced in Feb. 2000 that the Carilon product line is being discontinued. CARILON Polymer D26VM100 is a high-flow injection molding grade with mechanical properties which classify it as an .. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 190 °C |
60 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
M. Holland Company LD800 LDPE
(discontinued **) Features: High Clarity, High Flow, Narrow Molecular Wt. Dist., Good Processability, Warp ResistantUses: Closure Caps, Drink LidsApprovals: FDA 21 CFR 177.1520(c) 2.2 and ASTM D 1248, I, Class A, Cat.. |
|||
Melt Flow | 60 g/10 min | 60 g/10 min | ASTM D1238 |
Hyosung Topilene S905H PP S905H Fiber Grade HomopolymerApplications: SpunboundCharacteristics:High flowabilityProcessabilityInformation provided by Hyosung Corporation |
|||
Melt Flow | 60 g/10 min @Load 10.0 kg, Temperature 220 °C |
60 g/10 min @Load 22.0 lb, Temperature 428 °F |
ASTM D1238 |
LG Chemical AF342F ABS, Flame Retardant, High Flow Feature: Injection Molding, Flame Retardant, High FlowApplication: Electric/Electronic Applications (TV, Monitor Housing) IT/OA deviceCAS No. 9003-56-9, 40039-93-8 and 1309-64-4Information provided .. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 230 °C |
60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Inno-Comp INNOPOL® CS 2-9514 10% Talc-Filled, Elastomer Modified Polypropylene Block-Copolymer INNOPOL® CS 2-9514 is a 10% talc-filled, elastomer modified compound based on polypropylene block-copolymer. This grade is available in nature and custom colored form.INNOPOL® CS 2-9514 is dev.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 523 Linear Thermoplastic Polyurethane Pearlbond™ 523 is a linear, polycaprolactone-copolyester polyurethane, supplied in form of white spherical granules with a very high crystallization rate and a very high thermoplasticity level... |
|||
Melt Flow | 60 - 110 g/10 min @Load 21.6 kg, Temperature 170 °C |
60 - 110 g/10 min @Load 47.6 lb, Temperature 338 °F |
DDIN 53.735 |
Lubrizol Advanced Materials Pearlbond® DAP 750/2 Thermoplastic Polyurethane The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pelle.. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 260 °C |
60 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BKV 35 H2.0 EF 900116 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 275 °C |
60 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 260 °C |
60 g/10 min @Load 11.0 lb, Temperature 500 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Durethan® BKV 35 H2.0 EF 901510 Nylon 6, 35% Glass Fiber PA 6, injection molding grade, 35% glass fibers, good heat-ageing resistance, good flowability (easy flow) |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 123 Linear Thermoplastic Polyurethane Pearlbond™ 123 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines an extremely high crystallization rate with a very high thermoplasticit.. |
|||
Melt Flow | 60 g/10 min @Load 10.0 kg, Temperature 250 °C |
60 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® HR-1008B PC/ABS, Unreinforced PC/ABS material that can be used for hand phone and car phoneInformation provided by Samsung Cheil Industries. |
|||
Melt Flow | 60 g/10 min @Load 10.0 kg, Temperature 250 °C |
60 g/10 min @Load 22.0 lb, Temperature 482 °F |
ASTM D1238 |
Samsung Cheil Industries Infino® TN-1200 PC, Unreinforced FR Information provided by Samsung Cheil Industries. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 250 °C |
60 g/10 min @Load 4.76 lb, Temperature 482 °F |
ASTM D1238 |
Samyang Tribit® 1500G10 PBT, Reinforced General Purpose Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1500G10 is a reinforced, general purpose gr.. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 235 °C |
60 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238 |
Samyang Tribit® 1501N PBT, Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1501N is a V-2 flame retardancy grade.Appli.. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 230 °C |
60 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPR 12222 Random Copolymer Polypropylene Total Petrochemicals PPR 12222 is a high melt flow index, clarified random copolymer. Its high transparency makes it particularly suitable for the production of household articles and packaging. It.. |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 160 °C |
60 g/10 min @Load 4.76 lb, Temperature 320 °F |
cm<sup>3</sup>/10 min; ISO 1133 |
EMS-Griltech Griltex® D 1541A Copolyamide Hotmelt Adhesive (Apparel Interlinings) Description: GRILTEX adhesive products, either in pellet or powdered form, are used to coat apparel interlining substrates. Interlining substrates, coated with GRILTEX adhesive products, provides fo.. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 275 °C |
60 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 CF10 Polyamide 6 10% Carbon Fiber - Antistatic and Electroconductive Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Electroconductive grade based on carbon fiber reinforcement, very high stiffn.. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 275 °C |
60 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 TF10 Polyamide 6 - Improved Slip Properties Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid.. |
|||
Melt Flow | 60 - 75 g/10 min | 60 - 75 g/10 min | ISO 1133 |
Beijing Ranger Chem BLUESTAR® 1079 PBT Can be used directly for spinning, and producing color concentrates. It can also be used for production after reinforcement & compounding.Information provided by Beijing Ranger Chemical Co. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 300 °C |
60 g/10 min @Load 11.0 lb, Temperature 572 °F |
ASTM D1238 |
BLUESTAR LXS 109 PPE-PS Typical Applications: Electrical partsFire RatedInformation provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 275 °C |
60 g/10 min @Load 11.0 lb, Temperature 527 °F |
ISO 1133 |
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced 15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High.. |
|||
Melt Flow | 60 g/10 min | 60 g/10 min | ASTM D1238 |
Huntsman PE2072 Injection Molding Polyethylene
(discontinued **) Homopolymer and FDA compliant.Features: Very high flow rapid set-up characteristics, excellent clarity, gloss, and stiffness.Applications: Injection molding: lids and difficult to fill applications... |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
DDIN 53.735 |
Lubrizol Advanced Materials Pearlbond® D183 Thermoplastic Polyurethane
(discontinued **) The Pearlbond® grades are aromatic crystalline TPUs used for the production of heat activated shoe counters and toe puffs, and orthopedic products. The Pearlbond® grades are supplied in pellet fo.. |
|||
Melt Flow | 60 - 100 g/10 min @Load 2.16 kg, Temperature 170 °C |
60 - 100 g/10 min @Load 4.76 lb, Temperature 338 °F |
ISO 1133 |
Lubrizol Advanced Materials PEARLBOND® 103 Linear Thermoplastic Polyurethane Pearlbond™ 103 is a linear, polycaprolactone-based polyurethane, supplied in form of small white granules, which combines a very high crystallization rate with a very high thermoplasticity level. I.. |
|||
Melt Flow | 60 g/10 min @Load 5.00 kg, Temperature 270 °C |
60 g/10 min @Load 11.0 lb, Temperature 518 °F |
Estimated using room temperature density; ISO 1133 |
Lanxess Pocan® A 3131 000000 PBT+ASA, 30% glass fibers PBT+ASA, 30% glass fibers, injection molding, low tendency to warp, improved surface finish |
|||
Melt Flow | 60 g/10 min @Load 2.16 kg, Temperature 300 °C |
60 g/10 min @Load 4.76 lb, Temperature 572 °F |
ASTM D570 |
LG Chemical LUCON CP6067 PC+CNT+CF Description: Injection Molding, PC+CNT+CF, Electrostatic Dissipation, High Strength, High Flow & Good ProcessabilityApplication: Wafer Carrier Box, Conveyor belt bearing blockCAS No. 103598-77-2, 74.. |