Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 54 g/10 min @Load 10.0 kg, Temperature 190 °C |
54 g/10 min @Load 22.0 lb, Temperature 374 °F |
ISO 1133 |
Multibase TPSiV® 4200-80A Thermoplastic Elastomer FEATURES & BENEFITS: Soft silky feel; Excellent abrasion and scratch resistance; Excellent bonding to PC, ABS; Good chemical resistanceAPPLICATIONS: Solution for soft touch overmolding on consumer e.. |
|||
Melt Flow | 54 g/10 min @Load 5.00 kg, Temperature 200 °C |
54 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 54 g/10 min @Load 5.00 kg, Temperature 200 °C |
54 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-9 NSFG Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9 NSFG is a NSF 51 (food equipment) approved material suitable for a wide variety of applications. -NSF 51 approved -FDA (see Notes) -Overmold Adhesion to Polypropylene -Soft Touch,.. |
|||
Melt Flow | 54 g/10 min @Load 5.00 kg, Temperature 200 °C |
54 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7980-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7980-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Melt Flow | 54 g/10 min @Load 5.00 kg, Temperature 190 °C |
54 g/10 min @Load 11.0 lb, Temperature 374 °F |
|
Total Finaprene® 435 Styrene-Butadiene TPE Copolymer Compounded to 54 MFI
(discontinued **) Styrene-Butadiene CopolymerDescription: Finaprene® is a thermoplastic elastomer type radial styrene-butadiene block copolymer. Thanks to its medium molecular weight, Finaprene® 435 provides excel.. |
|||
Melt Flow | 54 g/10 min @Load 5.00 kg, Temperature 200 °C |
54 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Melt Flow | 54 g/10 min @Load 8.70 kg, Temperature 190 °C |
54 g/10 min @Load 19.2 lb, Temperature 374 °F |
ASTM D1238 |
Lubrizol Estane® MVT 80AF3 Thermoplastic Polyurethane, Moisture Vapor Transmission Type: Estane® MVT 80AF3 TPU is a aromatic polyether-based thermoplastic polyurethane (TPU).Features: High moisture vapor transmission, good low temperature properties and elasticity.Uses: Blown and.. |
|||
Melt Flow | 54 g/10 min @Load 2.16 kg, Temperature 230 °C |
54 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
ExxonMobil PP7075L1 Polypropylene Impact Copolymer Product Description: A nucleated impact copolymer resin with high flow and antistatic properties. It is suitable for molding applications like disposable houseware, consumer products, toys and rigi.. |