Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 420 g/10 min @Load 2.16 kg, Temperature 190 °C |
420 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 7710 Adhesive Application Resin Escorene Ultra UL 7710 is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt .. |
|||
Melt Flow | 420 g/10 min @Load 2.16 kg, Temperature 190 °C |
420 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil Escorene® UL 7710E Adhesive Application Resin Escorene Ultra UL 7710E is a very high flow, 26.7% vinyl acetate copolymer that has very good compatibility with hydrocarbon and natural tackifiers and most waxes. It is suitable for making hot melt.. |