Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.50 - 8.20 g/10 min | 4.50 - 8.20 g/10 min | Average value: 5.73 g/10 min Grade Count:3 |
Overview of materials for Acrylonitrile Butadiene Styrene (ABS), PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile Butadiene Styrene (ABS), PTFE Filled". Each property range of values reported is minimum a.. |
|||
Melt Flow | 4.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1227D Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1479 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1479F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.50 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.50 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1479-L3 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1123 BLK 111 Thermoplastic Elastomer Uses: General Purpose; Grommets; Weather Stripping Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 1.. |
|||
Melt Flow | 4.50 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.50 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Uniprene® UN-7100-64 Thermoplastic Vulcanizate Notes: Injection Rate: Fast Uses: Expansion Joint; Grommets; Tubing; Gaskets; Plugs; Weatherstripping; Glazing; Shock Absorbing Pads Forms: Pellets Processing Method: Extrusion; Injection Molding Ex.. |
|||
Melt Flow | 4.50 - 55.0 g/10 min | 4.50 - 55.0 g/10 min | Average value: 17.8 g/10 min Grade Count:22 |
Overview of materials for Polycarbonate, PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app.. |
|||
Melt Flow | 4.50 - 150 g/10 min | 4.50 - 150 g/10 min | Average value: 39.0 g/10 min Grade Count:40 |
Overview of materials for Polyethersulfone (PES) This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone". Each property range of values reported is minimum and maximum values of appropriate M.. |
|||
Melt Flow | 4.50 - 25.0 g/10 min | 4.50 - 25.0 g/10 min | Average value: 10.6 g/10 min Grade Count:5 |
Overview of materials for Polyethersulfone (PES), 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyethersulfone (PES), 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% .. |