Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 400 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 752 °F |
ASTM D1238 |
Oxford Polymers PEEK 450-INJ-Black PEEK Product Description: Polyetheretherketone, general purpose injection molding grade Processing and Delivery Form: Pellets and Injection MoldingAdditives: Carbon black Special Characteristics: Precol.. |
|||
Melt Flow | 4.00 - 60.0 g/10 min | 4.00 - 60.0 g/10 min | Average value: 23.0 g/10 min Grade Count:41 |
Overview of materials for Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), 10% Glass Fiber Filled".Specific grades with glass content between 5% .. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1871R Thermoplastic Elastomer Notes: USP Class VI; ISO 10993; Clear Features: Good Stability Uses: Medical TubingInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1473F Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1564-L1 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1564L2 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2100 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2260 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP 1564 Thermoplastic Elastomer Notes: Translucent Features: High FlowInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2830E Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 - 20.0 g/10 min @Load 21.6 kg, Temperature 200 °C |
4.00 - 20.0 g/10 min @Load 47.6 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Sinpolene MBB2185 High Impact Polystyrene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Carbon Black (300000 ppm) Forms: Pellets Features: General PurposeInformation Provided by Teknor Apex |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 1383N Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® OBC 2318D Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2318G Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets .. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Teknor Apex Telcar® TL-2365A Thermoplastic Polyolefin Elastomer Uses: Automotive Applications; Flexible Grips; Gaskets; General Purpose; Industrial Applications; Roof Vents Forms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Injectio.. |
|||
Melt Flow | 4.00 g/10 min @Load 5.00 kg, Temperature 200 °C |
4.00 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-1878 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.00 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Teknor Apex Monprene® MP-2604B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Melt Flow | 4.00 - 20.0 g/10 min | 4.00 - 20.0 g/10 min | Average value: 11.1 g/10 min Grade Count:16 |
Overview of materials for Polypropylene with 30% Mica Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Mica Filler". Specific grades with primary filler content between 25% and 34% are.. |
|||
Melt Flow | 4.00 - 48.0 g/10 min | 4.00 - 48.0 g/10 min | Average value: 21.0 g/10 min Grade Count:11 |
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum .. |