Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Multibase Multi-Pro® 1004 R Polypropylene Features: Scratch Resistance, GoodHeat Resistance, HighStiffness, GoodForms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Melt Flow | 4.0 - 8.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 - 8.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom PLASTALEN® EH 91 N Polyethylene HDPE regrind for injection molding. General use in all industry branches. Delivered in blue ( approx. RAL 5015) mode.Information Provided by Plastcom spol. s r.o. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 66 BT Polyamide 66 FeaturesModified for general use, with excellent manufacturing properties, characterized by high strength and toughness also at low temperatures. Use in automotive, electrical, engineering and cons.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
SABIC PS 330 High Impact Polystyrene for Sheet Extrusion Product Description: High Impact Polystyrene PS 330 is manufactured by continuous mass polymerization of styrene monomer. An elastomer is incorporated during polymerization to achieve impact resis.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | Condition G |
Ineos Nova 4211 Medium Impact Polystyrene
(discontinued **) Excellent balance of properties, USP Class VIApplications: Consumer electronics, Injection molding applicationsProperties were determined on injection molded specimens at 23°C and 50% R.H. unless o.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 330 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 626 °F |
|
Covestro Apec® DP 1-9389 Polycarbonate
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and ha.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 330 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 626 °F |
ASTM D1238 |
Covestro Apec® DP9-9371 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | 230/2.16 (typical); ASTM D1238 |
Fiberfil® PP-62/MI/25 Polypropylene Copolymer, 25% Mica Reinforced Information provided by FIBERFIL Engineered Plastics |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
LyondellBasell Hostacomâ„¢ AE716BC Polypropylene Homopolymer Description: Hostacomâ„¢ AE716BC conventional melt flow, 1,400 MPa flexural modulus, UV-stabilized, 40% calcium carbonate-filled polypropylene homopolymer has a good balance of properties and pro.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Techmer ES HiFill® PP 0112 B Polypropylene Availability: North AmericaForms: PelletsFiller/Reinforcement: Unspecified Filler/ReinforInformation provided by TP Composites, Inc. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
SCG Chemicals EL-Leneâ„¢ M3504DXP Octene (C8) Rotational Molding Resin Natural base resin available in powder formKey Characteristics:Excellent ESCRExcellent impact resistanceLow warpageFair processingTypical Applications: Chemical storage tanks, diesel tanks, spray t.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis MG7547S Polyethylene MG7547S is a high-density polyethylene produced by a low pressure process. This grade has an excellent impact strength and low distortion even at low temperatures. It also contains UV stabilizer, wh.. |
|||
Melt Flow | 4.0 - 12 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 12 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 - ISO 1133 |
DuPont Elvaloy® HP441 Ethylene/N-Butyl Acrylate/Carbon Monoxide Copolymer Specialized copolymers deliver flexibility, toughness and weatherability to adhesives, plastics, highways and roofing.Availability: GloballyInformation provided by DuPont. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ FPP 3460 Glass-Mineral Hybrid Filled Copolymer DescriptionPolyfort® FPP 3460 is a 40% glass-mineral hybrid filled copolymer.Information provided by A. Schulman. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total LDPE LD 0304 Low Density Polyethylene - Extrusion Coating LDPE LA 0304 is a low density polyethylene made by a high pressure autoclave process without antioxidant.Application examples: coating of paper, paperboard, aluminum.Information provided by Total Pe.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Polyram RamTal PM3009G5 Acetal, 25% Glass Fiber 25% Glass fiber reinforced polyacetal for injection molding applications.Information provided by Polyram Ram On Ind. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
UBE UMERIT 500F Metallocene LLDPE Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical propert.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 420401S SBS Based Material, 40D Hardness, Natural The 400S-series is a good alternative for indoor applications and disposable articles that do not have high requirements for ageing and heat resistance. The raw materials are specially selected for.. |
|||
Melt Flow | 4.0 - 8.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 - 8.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Ex-Tech Plastics RenewTech™ BioPlastics Ingeo™ PLA Derived from annually renewable resources, RenewTech™ BioPlastics 7000 sheet is made with Ingeo™ PLA biopolymer as a base, giving you a packaging solution with competitive cost value performance c.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133 |
DSM Arnitel® XG6029 TPC-ET Extrusion Grade |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Arkema Group Pebax® 7233 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Aclo Accutech Nylon 6 NY0730G30L Glass Reinforced |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM-D1238 |
Braskem H 503HS HOMO Polypropylene Homopolymer H 503HS is a low melt flow rate homopolymer for general purpose. It is designed for raffia extrusion and fiber extrusion. This product exhibits excellent processability, high speed production with g.. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Braskem MR 435 UV LMDPE Rotational Molding Polyethylene Applications: Water tanks; toys; automotive components. Information provided by Braskem |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-30FG-0877A 30% Glass Fiber Reinforced, UV Stabilized Information provided by Asahi Thermofil |
|||
Melt Flow | 4.0 - 6.0 g/10 min @Load 10.0 kg, Temperature 230 °C |
4.0 - 6.0 g/10 min @Load 22.0 lb, Temperature 446 °F |
ASTM D1238 |
3M Dyneon™ PVDF 2066_0002 Fluoroplastic 3M™ Dyneon™ PVDF 2066/0002, a fluoropolymer material, provides an excellent balance of physical properties, processability, surface smoothness, flexibility, and refractive index, allowing for a wi.. |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Copolymer CP0436G20M10CL Glass/Mineral Reinforced Coupled |
|||
Melt Flow | 4.0 g/10 min | 4.0 g/10 min | MFI condition not specified |
Chem Polymer Formax 604 Acetal, Low Flow A 4 melt flow index copolymer acetal for extrusion or thick injection molding applications.Data provided by the manufacturer, Chem Polymer. |
|||
Melt Flow | 4.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
4.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products GC30P104-00 30% Glass Fiber Reinforced Polypropylene, Chemically Coupled, Natural Applications: BracketsHead lamp housingsBattery trayInjection molding conditions reported in table.Information provided by RheTech Products. |