Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 35 g/10 min @Load 1.20 kg, Temperature 300 °C |
35 g/10 min @Load 2.65 lb, Temperature 572 °F |
Procedure A Condition 0; ASTM D1238 |
Network Polymers NPP 3514 Description: Black Polycarbonate Polyester AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 35 g/10 min @Load 1.20 kg, Temperature 300 °C |
35 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL1810T PC Copolymer (Europe-Africa-Middle East) Lexan* EXL1810T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers cold temperature (0 °C) ductility in combination with very high flow char.. |
|||
Melt Flow | 35 g/10 min @Load 1.20 kg, Temperature 300 °C |
35 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® EXL1890T PC Copolymer Lexan* EXL1890T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade for food contact applications. This resin offers cold temperature (0 °C) ductility in combin.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH350V Polypropylene, Homopolymer, Extrusion Coating, Spunbound, Gas Fade & UV Resistant COPYLENE™ CH350V is a very high melt flow polypropylene homopolymer resin designed for fiber spinning. Applications: Food Packaging Film, Heavy Duty Packaging, Absorption & Filtration, Filament Yar.. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | Condition L 230/2.16; ASTM D1238 |
Pinnacle Polymers 2135 H Medium Impact Polypropylene Copolymer, Injection Molding Grade This Pinnacle Polymers Polypropylene is made via UNIPOL™ PP technology, which utilizes gas-phase fluidized bed reactors with a high activity catalyst system to ensure uniform physical properties an.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Phillips 66 COPYLENE® CH350 Polypropylene Homopolymer COPYLENE™ CH350 is a controlled rheology, barefoot homopolymer designed for application as a base resin for compounding, consumer products and other injection molding applications.Applications: Inj.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax SD242 Polypropylene Impact Copolymer Key Features: short cycle times for high productivity, good cold impact resistance, good stiffness and impact balance, high flow ease of mold filling and minimum warpage, low odor and low taste tran.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
LyondellBasell Pro-fax SV954 Polypropylene Impact Copolymer Key Features: nucleation shortens cycles for higher productivity, resists dirt and dust pick-up, good cold impact resistance, good stiffness and impact balance, high flow for ease of mold filling an.. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
Flint Hills AP6835-HS Polypropylene Impact Copolymer Features: Excellent processing, good low temperature impact strength.Applications: Injection molding: Appliance components, consumer durables and closuresInformation Provided by Flint Hills Resource.. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
Flint Hills P4C6B-194 Polypropylene Homopolymer Features: Antistat, Nucleated. Product does not contain animal derived components. Phthalate-free.Applications: Injection MoldingInformation Provided by Flint Hills Resources |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H35G-GP Polypropylene Homopolymer This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsC.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Ineos H35Z-00 Polypropylene Homopolymer This is a high flow rate, nucleated and antistatic homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 C.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Multibase Multi-Flex® A 8502 A Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Melt Flow | 35 g/10 min @Load 10.0 kg, Temperature 220 °C |
35 g/10 min @Load 22.0 lb, Temperature 428 °F |
from MVR; ISO 1033 |
Sax Polymers SAXLAC 835U Acrylonitrile Butadiene Styrene Saxalac 835U is an antistatic, easy flowing light stabilized ABS injection molding grade, characterized by high impact strength, high stiffness and good resistance to heat distortion.Mechanical prop.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PX 1040 Information provided by A. Schulman. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
A. Schulman POLYFORT™ PX 1040 Information provided by A. Schulman. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
A. Schulman PP 2268-01 Polypropylene High Flow, Impact Copolymer Polypropylene DescriptionPolypropylene PP 2268-01 is an automotive recognized high flow impact copolymer polypropylene.ApplicationPP 2173-01 is intended for use in interior trim applications.Information provided .. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM D1238 |
A. Schulman PP 3479-01 Polypropylene Random Copolymer DescriptionPolypropylene PP 3479-01 is a polypropylene random copolymer produced utilizing unique catalyst and processing technology. It was designed for injection molding and stretch blow molding .. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 190 °C |
35 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Green P30244/4 Concentrate Based In Copolymer PP DescriptionPOLYBATCH® P30244/4 is a green color concentrate based in Copolymer PP. This concentrate was designed to provide color in blow molding applications. POLYBATCH® P30244/4 is typically .. |
|||
Melt Flow | 35 g/10 min @Load 5.00 kg, Temperature 230 °C |
35 g/10 min @Load 11.0 lb, Temperature 446 °F |
ISO 1133 |
ELASTO UK Dryflex® 3037-111 TPE, Modified Injection Molding Grade for Auto Interior Parts The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. VTC Dryflex® 3037-111 is specifically designe.. |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ISO 1133 |
CTC X-PRO CTC PP 2040 Polypropylene Copolymer X-PRO PP 2040 is a high melt polypropylene copolymer. It has applications in general purpose industrial, housewares, and construction.Data provided by Composite Technologies (CTC). |
|||
Melt Flow | 35 g/10 min | 35 g/10 min | ASTM-D1238 |
CTC X-PRO CTC PP1035 Polypropylene Homopolymer X-PRO PP 1035 is a polypropylene homopolymer. Its applications are: general purpose industrial injection molding, virgin polypropylene diluents, and polymer base for glass, talc or specialty filled.. |
|||
Melt Flow | 35 g/10 min @Load 5.00 kg, Temperature 265 °C |
35 g/10 min @Load 11.0 lb, Temperature 509 °F |
ASTM D1238 |
Diamond Polymers ASAPC 6040 UV Stabilized Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D 1238 |
Cossa Polimeri ESTAPROP KUR 4000 CH/TD Polypropylene Copolymer Polypropylene copolymer, elastomer modifiedInformation provided by Cossa Polimeri S.r.l. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem F350HC2 High Crystallinity Homopolymer Polypropylene Description: Very High Flexural ModulusApplications: Suggested Uses Include Compounding, Automotive, AppliancesThis resin meets the requirements for olefin polymers as defined in 21 CFR, section 177.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Braskem TR3350UC Random Copolymer Polypropylene Description: Maximum see-through clarity, minimal haze; superior color stability, process stability, and gloss; low odor, high melt flow.Applications: Suggested uses; reusable food containers, house.. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 250 °C |
35 g/10 min @Load 4.76 lb, Temperature 482 °F |
ISO 1133 |
BASF Ultradur B 4300 G2 LS High Speed BK15045 10% Glass Filled PBT |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
RheTech Products HP501-01 High Performance Polypropylene Copolymer, Non-UV Stabilized, Black Applications: Battery traysInterior TrimInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Melt Flow | 35 g/10 min @Load 2.16 kg, Temperature 230 °C |
35 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Chase Plastics CP Pryme® PPC100-35M Polypropylene Copolymer Information provided by Chase Plastics. |