Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | (Condition L) ASTM D-1238 |
Multibase Multi-Flex® TPE G 7940 GRAPHITE Ash is 7.3%. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | ASTM D1238 |
ExxonMobil Escorene® LD 767.MJ Blown Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | ASTM D1238 |
ExxonMobil Escorene® LD 767.MJ Cast and Compounding Film Resin
(discontinued **) Escorene Ultra LD 767.MJ is a low gel 29.5% vinyl acetate copolymer designed for film and compounding applications.Information provided by ExxonMobil Chemical |
|||
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | ASTM D1238 |
ExxonMobil Escorene® LD 767.MJ Molding, extrusion and compounding resin
(discontinued **) Escorene Ultra LD 767.MJ is a high viscosity, 29.5% vinyl acetate copolymer suitable for making very soft, blow molded or extruded articles with very good low temperature toughness. It can also be .. |
|||
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | Exxon Method |
ExxonMobil Escorene® LD-767 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A low gel 29.5% vinyl acetate copolymer designed for film and compounding applications. The resin provides very low modulus films with high tensile.. |
|||
Melt Flow | 3.1 g/10 min | 3.1 g/10 min | ASTM D1238 |
LyondellBasell Plexar® PX1007 Extrudable Tie-Layer Resin - Anhydride Modified EVA ApplicationsPlexar® tie-layers are chemically modified resins used to bond unlike materials, primarily in packaging and industrial applications. Common adherents include polyethylene resins and .. |
|||
Melt Flow | 3.1 - 3.5 g/10 min @Load 2.61 kg, Temperature 190 °C |
3.1 - 3.5 g/10 min @Load 5.75 lb, Temperature 374 °F |
ASTM D1238 |
LG Chemical SEETEC BS500 LDPE Characteristics: Good Processability and Good cell uniformity& stability Additives: Antioxidant, Antiblocking agent, Slip AgentApplications: Foam sheetInformation provided by LG Chemical |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Styrenics Polystyrene 476M (NAFTA) High-impact grade of polystyrene with good ESCR designed to provide uniform melt flow for excellent processability.Information provided by BASF.Ineos Styrenics purchased this product line from BASF .. |
|||
Melt Flow | 3.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
3.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 4000 PEI Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Melt Flow | 3.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
3.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM 4000 PEI (Asia Pacific) Glass fiber, PTFE, and Graphite filled, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0 listing. |
|||
Melt Flow | 3.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
3.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5201R PEI 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Melt Flow | 3.1 g/10 min @Load 6.60 kg, Temperature 337 °C |
3.1 g/10 min @Load 14.6 lb, Temperature 639 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM CRS5201R PEI (Asia Pacific) 20% Glass fiber filled, standard flow Polyetherimide copolymer (Tg 225C) with internal mold release and enhanced chemical resistance to strong acids, bases, aromatics, and ketones. ECO Conforming. |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D 1238 |
Styrolution PS 6200/6201 HIPS Excellent toughnessDesigned for deep draw thermoformingUSP Class VI certifiedInformation provided by Styrolution |
|||
Melt Flow | 3.1 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.1 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM D1238; ISO 1133 |
Styron MAGNUM™ 3325 SLG Acrylonitrile Butadiene Styrene (ABS) Resin Overview: Super Low Gloss, Medium Heat, Medium Impact ABS resin for injection molded automotive interior trim applications Magnum 3325 SLG can achieve 60° Gardner gloss levels below 2.0 with low .. |
|||
Melt Flow | 3.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
DuPont Bynel® 4109 Anhydride-Modified LLDPE Adhesive Resin Bynel® Series 4100 resins are anhydride-modified, linear low-density polyethylene (LLDPE) resins. All 4100 Series resins are available in pellet form for use in conventional extrusion and coextrusi.. |
|||
Melt Flow | 3.1 g/10 min @Load 2.16 kg, Temperature 235 °C |
3.1 g/10 min @Load 4.76 lb, Temperature 455 °F |
ASTM D1238R |
UBE UBESTA® 3030UFX1 Rigid Industrial Grade Nylon 12 Description: UBE UBESTA® Industrial grade Nylon 12Comments: UV resistance, heat resistanceInformation provided by UBE. |
|||
Melt Flow | 3.1 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.1 g/10 min @Load 2.65 lb, Temperature 572 °F |
ISO 1133 |
Covestro Makrolon® 6717 Polycarbonate, Flame Retardant Grade ISO 7391-PC,MFLR,(,,)-05-9Global gradeFormerly Makrolon DP1-1853MVR (300 °C/1.2 kg) 3.0 cm3/10 minFlame retardantUL 94V-0/2.0 mmHigh viscosityBranchedUV stabilizedEasy releaseInjection molding - Me.. |
|||
Melt Flow | 3.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
ExxonMobil LDPE LD 144BR Low Density Polyethylene Resin Product Description: LD 144BR is an LDPE grade, which offers excellent optical properties combined with increased stiffness and drawdown properties.Availability: Africa & Middle East and Europe Addi.. |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Entec Hyrene® PS-HI 3/3 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Melt Flow | 3.1 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.1 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Entec Hyrene® PS-HI 3/4 High Impact Polystyrene Available in North America Features: High Impact ResistanceRoHS Compliant Form: Pellets Information provided by Entec |
|||
Melt Flow | 3.1 g/10 min @Load 10.0 kg, Temperature 235 °C |
3.1 g/10 min @Load 22.0 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Conditioned) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Melt Flow | 3.1 g/10 min @Load 10.0 kg, Temperature 235 °C |
3.1 g/10 min @Load 22.0 lb, Temperature 455 °F |
|
Arkema Group Rilsan® BESN P40 TL Nylon 11, Flexible Tubing Grade (Dry) Designation ISO 1874-PA11-P,EHL,22-003Flexible grade for tubes extrusion. Available color: black and natural. Light and heat stabilized.High flexibility. High impact strength. Very good chemical res.. |
|||
Melt Flow | 3.1 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.1 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Total Lumicene® mPE M 3427 Metallocene Polyethylene, Cast Film Lumicene® mPE M 3427 is a second generation metallocene based Polyethylene with hexene as comonomer.Lumicene® mPE M 3427 can be processed at high output rates with low extrusion pressure, low neck.. |