Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 3.0 g/10 min @Load 0.325 kg, Temperature 270 °C |
3.0 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 66 GF 50 LS PA66, 50% glass fibre, light stability FeaturesChemically reinforced with 50% glass fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry, l.. |
|||
Melt Flow | 3.0 g/10 min @Load 1.00 kg, Temperature 235 °C |
3.0 g/10 min @Load 2.20 lb, Temperature 455 °F |
Procedure A Condition Q; ASTM D1238 |
Network Polymers Softflex® 8800 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
PolyOne Dynaflex™ G7950-1001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7950-1001-00 is an easy processing, general purpose material designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypro.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
STN EN ISO 1133 |
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con.. |
|||
Melt Flow | 3.0 g/10 min @Load 0.325 kg, Temperature 270 °C |
3.0 g/10 min @Load 0.716 lb, Temperature 518 °F |
|
Plastcom SLOVAMID 6 NG GF 45 PA6, 45% glass fibre FeaturesPA 6 for injection moulding, chemically strengthened with 45% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-good.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Ineos Nova 474 High Performance Styrenic Enhanced Polystyrene
(discontinued **) Custom ColorsApplications: Injection molding, Alternative to engineering resinsPerformance grades of polystyrene are engineered to have specific properties. These products can be custom colored. N.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
LyondellBasell Lupolen® 5261 Z Q 456 B High Density Polyethylene, Pipe and Sheet Extrusion Grade Lupolen 5261 Z Q 456 B is a high density polyethylene (HDPE) with high melt viscosity for ram extrusion of peroxide crosslinked pipes (PE-Xa). The product is supplied as a nominal 20 mesh (840 um) p.. |
|||
Melt Flow | 3.0 g/10 min @Load 10.0 kg, Temperature 200 °C |
3.0 g/10 min @Load 22.0 lb, Temperature 392 °F |
ASTM D1238 |
Techmer ES Electrablend® HIPS Availability: North AmericaForms: PelletsFeatures: ConductiveInformation provided by TP Composites, Inc. |
|||
Melt Flow | 3.0 - 9.0 g/10 min @Load 5.00 kg, Temperature 230 °C |
3.0 - 9.0 g/10 min @Load 11.0 lb, Temperature 446 °F |
ASTM D1238 |
Solvay Specialty Polymers Solef® 21510 Polyvinylidene Fluoride (PVDF) Solef® 21510 PVDF copolymer has medium viscosity and is suitable for extrusion and for solution processing in lithium batteries applications.Features: Copolymer; Good Flexibility; Medium Viscosit.. |
|||
Melt Flow | >= 3.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
>= 3.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
ISO 1133 |
Styrolution Absolac® XT04P ABS High heatInformation provided by Styrolution |
|||
Melt Flow | 3.0 g/10 min @Load 10.0 kg, Temperature 220 °C |
3.0 g/10 min @Load 22.0 lb, Temperature 428 °F |
|
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS Information provided by Polymer Technology and Services, LLC (PTS). |
|||
Melt Flow | 3.0 g/10 min @Load 3.80 kg, Temperature 230 °C |
3.0 g/10 min @Load 8.38 lb, Temperature 446 °F |
ASTM Data |
Styron Pulse® 830 ABS + Polycarbonate PULSE® 830 Engineering resin offers excellent processability, high heat resistance, and high impact strength at both room and low temperatures.PULSE 830 Engineering resin has been used in automot.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ISO 1133 |
Styrolution PS 158K GPPS Styrolution PS 158K is a heat resistant, rapid freezing general purpose grade. It is suitable for expanded sheet and film; for blends with high impact Styrolution PS in heat contact applications; fo.. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ISO 1133 |
Borealis Borclear™ RC707MO Polypropylene Borclear™ RC707MO is intended for blow molding. This grade provides high gloss, high transparency and excellent impact properties. This grade also features high heat distortion temperature. Applic.. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Teknor Apex Telcar® TL-2635D Thermoplastic Elastomer Uses: Building Materials; Flexible Grips; General Purpose; Handles; Safety Equipment; Toys Injection Notes: Injection Rate: Moderate-Fast Extrusion Notes: Screw Speed: 30 to 100 rpmInformation Provi.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ISO 1133 |
Borealis Himod™ FT7294 LDPE for Film Himod FT7294 is a tubular, low-density polyethylene grade for the production of packaging films. Compared to standard LDPE grades, the Himod products provide a combination of higher stiffness and i.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 190 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
A. Schulman POLYBATCH™ Brown 10306 Concentrate Based In Polyethylene DescriptionPOLYBATCH® 10306 is a brown color concentrate based in linear low density polyethylene. This product was formulated to offer color and opacity in polyethylene film applications. POLYBA.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Total PPH 4054 Polypropylene Homopolymer Polypropylene PPH 4054 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min.Polypropylene PPH 4054 has been designed for the production of BOPP film with the tenter frame process. Th.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Total PSI 825EX Polystyrene Polystyrene 825EX is a high impact polystyrene designed for high stiffness in extrusion/thermoforming applications. The balance of high stiffness and impact properties allow for light weighting of t.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D-1238 |
Chevron Phillips MB3150 Crystal Polystyrene High heat crystal polystyrene.Applications:Compact disc jewel boxesConsumer containers, vials, jars, etc.Desk organizersAudio cassettesFeatures:Fast cycling due to high heat distortionHigh Vicat sof.. |
|||
Melt Flow | 3.0 g/10 min @Load 5.00 kg, Temperature 190 °C |
3.0 g/10 min @Load 11.0 lb, Temperature 374 °F |
ASTM D1238 |
ELASTO UK Dryflex® 650700 TPE, Improved Compression Set and High Temperature Resistance, 70A Hardness The VTC TPE Group have developed endless formulations to fulfill different properties and application requirements to optimize the finished component. This grade is designed with improved compressi.. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
ExxonMobil Escorene™ UL 00328 Ethylene Vinyl Acetate Copolymer (European Grade) Product Description: UL 00328 is a copolymer of ethylene and vinyl acetate.Availability: Africa & Middle East and Europe Additive: Antiblock: NoSlip: No Thermal Stabilizer: No Applications: Compoun.. |
|||
Melt Flow | 3.0 g/10 min @Load 2.16 kg, Temperature 230 °C |
3.0 g/10 min @Load 4.76 lb, Temperature 446 °F |
ASTM D1238 |
Diamond Polymers NPP25-0303 GF20 20% Glass Filled Polypropylene Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Melt Flow | 3.0 g/10 min @Load 1.20 kg, Temperature 300 °C |
3.0 g/10 min @Load 2.65 lb, Temperature 572 °F |
|
Covestro Makrolon® 1143 Polycarbonate Pseudoplastic behavior and high viscosity extrusion grade with UV stabilizer and easy mold release, special grade for twin-wall sheet.Information provided by Bayer.As of 1 September 2015, Bayer Mate.. |
|||
Melt Flow | 3.0 g/10 min | 3.0 g/10 min | ASTM D1238 |
Aclo Accutech Polypropylene Homopolymer HP0336G20M10CL Glass/Mineral Reinforced Coupled |
|||
Melt Flow | 3.0 - 7.0 g/10 min | 3.0 - 7.0 g/10 min | |
Asahi Glass Fluon® P-805UP PFA Perfluoropolymer Fluon® PFA is a copolymer of tetrafluoroethylene (C2F4) and perfluoroalkoxyethylene, which has excellent chemical, electrical, mechanical and surface properties. PFA retains many inherent character.. |
|||
Melt Flow | 3.0 - 12 g/10 min @Load 5.00 kg, Temperature 200 °C |
3.0 - 12 g/10 min @Load 11.0 lb, Temperature 392 °F |
ASTM D1238 |
Aaron Industries AAROLENE® ARPS HI 100-3 Polystyrene Compounded Resin AAROLENE® ARPS 100 Series Polystyrene Compounded ResinColor may be specified. Melt Flow Index may be specified. |